Tips to get better arc welding


December 7th, 2009

Shielded Metal Arc Welding is otherwise known as stick or arc welding. There are 5 most important aspects that will influence your arc welding effectiveness. They are
- Current setting
- Length of arc
- Angle of electrode
- Manipulation of the electrode
- Speed of travel
The above listed 5 will help you improve your welds particularly if you are a newbie. If you are still thinking about which machine to buy then these below listed tips will help you decide if you should buy this welder or not.
- For an all purpose welding utility you can go in for Miller’s Thunderbolt. A DC powered machine is more advantageous than an AC powered one as it starts easily, produces less spatter and smooth arcs are possible too.
- Some brands produce machines that are capable of an amperage and duty cycle inversely proportional to each other.
This method does not demand strenuous cleaning routine.

Share
1 Star2 Stars3 Stars4 Stars5 Stars (No Ratings Yet)
Loading ... Loading ...

Tags: ,

2 Responses to “Tips to get better arc welding”

  1. arvind says:

    we have some problems while welding that is when 0.5 mm steel is welded to make containers it gets burnt at edges i want a solution to that

  2. loans says:

    Blogs Very informative article. I’ve found your blog via Yahoo and I?m really glad about the information you provide in your posts. Thank You for sharing this very informative article… Regards

Leave a Reply