Mistakes are so intolerable in the field of welding. It is wise to check as much as possible before making a weld if you are on the right track. Inspecting in this manner will lead to lessening any probabilities of costly expenses. Follow the maintenance suggestions to make your plasma cutter last long.
- Do replace consumable parts as advised by the manufacturer. Or grab some suggestions from your manufacturer for the purpose.
- Assemble the torch perfectly along with other consumables. This will lead to an efficient working of the equipment.
- Use the exact parts in your cutter depending upon the plasma gas used and the cutting amperage.
- Ensure that appropriate gas and coolant flow through to ensure better life spans of consumables.
- Shun unnecessary use of o-ring lubricant and anti spatter compounds.
- Keep away from using the torch like a hammer.
- Stay away from stretching arc. Otherwise life span of your consumable will lessen at a great speed.
- Keep the torch clean by using hydrogen peroxide to do the magic.
Tags: Plasma Cutters, plasma cutting, plasma cutting machine




Hi, I found your blog on msn. I’m pretty happy to have found your blogbecause I think it is interesting! Really good content. Ruth
I have been reading the articles on this site for sometime. This is my first comment. Your blog has been very useful for me and it provides very good content.
I found your blog on google and read a few of your other posts. I just added you to my Google News Reader. Keep up the awesome work Look forward to reading more from you in the future.