Overview of TIG Welding

TIG welding has had many names and because it started in the 1941s many older welders may refer to it as “heliarc” welding. This welding was initially used in the war efforts to weld airplanes because it did a good job on aluminum, magnesium, and stainless steel.

The reason it was called “heliarc” is because it needed an inert gas as a shielding gas and helium was what was available at that time. As people began to experiment with inert gases they found that Argon was a better choice than helium because it is a heavier gas and had less flow rate than helium.

TIG welding
has been found to be a better choice for flat welding because of its even flow. It was also found that TIG welders were able to make a more stable arc and getting the arc going was easier. It is also important to note that the name was changed to TIG but no one actually knows why or when this happened.

Tuesday, February 23, 2010

Safety measures while using plasma cutters

Plasma cutting involves large amount of attention and proper precautionary measures should be taken to ensure the safety of the people handling the job. Protective measures taken during general welding is not enough for plasma cutting. This is because the plasma cutter output voltages are much greater than welding voltages.

While operating a plasma cutter, electric circuit is formed between the torch, work piece and anything that comes into contact with the work piece. So when the plasma system is operating, you must never touch the work piece or the torch body. You are advised to wear insulated gloves and boots during plasma cutting process. You must keep yourself and your clothing dry and also make sure that you are not keeping contact with any wet surfaces while using the cutters.

The plasma cutter arc rays are extremely harmful as it releases intense visible and invisible rays that are dangerous to skin and eyes. Direct exposure to the rays would cause retina trouble and the UV rays emitted would affect your skin. You must wear gloves, safety shoes and hat along with flame resistant clothing which covers all exposed areas in your body.

During high amperage operations, the plasma cutters produce excessive noises. In that case, proper ear protection should be taken. During plasma arc cutting, toxic fumes and gases that drain oxygen is released. This can lead to serious injuries. In order to prevent the mishap, the cutting area should be well ventilated. Otherwise you can also use an approved air supplied respirator. Those who are wearing pace makers or hearing aids should be cautious while going near plasma cutters. It is advisable to consult a doctor before going near the processes.

However, plasma cutting is not a life hazard process. If you are taking appropriate safety measures, the process can be easily managed.
Visa Mastercard American Express Discover eCheck PayPal
Copyright 2004 - 2010 Everlast Power Equipment Inc. All Rights Reserved.

Diesel Generators | Multi-Purpose Units | Plasma Cutters | Welders | TIG Water Coolers | SAFETY Helmets Icon | Consumables | Spare Parts | Accessories | Welders Word Press | Welders News | Sitemap | Welder Blog | Welding Equipment Blogspot | Welding Supply Articles | Welding Calculators | Welding Symbols | Welding Terms | Welding Terms Finder | Welders Schools

Archieves - May 2009 | June 2009 | August 2009 | September 2009 | February 2010 | March 2010 | April 2010
While welding is a valuable skill to possess, it is important to get the right machine to do the job. If you are a professional or a hobbyist and are trying to find the machine to fit your needs, Everlast can help. We offer a full line of welders for the hobbyist and professionals, including MIG, TIG, STICK and plasma cutters. We are proud to feature IGBT components and modules from Siemens for long life service whether in the field, in the shop or in the home. Don't forget about our line of silent diesel generators and engine drive welders. We offer convenient ordering capability without leaving your home or office.