Security advices for Hose OR Gas Tubing:

Tuesday, March 8th, 2011

Use the right cooler hose for oxygen (green/black) and acetylene (red) and by no means use oxygen hose for acetylene or vice versa. Forever defend hose from being compressed on or run over. Avoid tangle and kinks. By no means leave the hose so that it can be tripped over. Hose connections shall be made through considerable fittings and clamped or otherwise securely fastened to these connections in such a way as to endure with no leakage a pressure twice as great as the maximum delivery pressure of the pressure regulators provided on the scheme.

Guard the hose from flying flickers, hot slag, hot work piece and open fire. If dust goes into hose, blow through (with oxygen, not acetylene) previous to coupling to torch or regulator. Store hose on a reel (an automobile wheel will do) when not in use. By no means permit the hose to come into contact with oil or grease; they deteriorate the rubber and comprise a hazard with oxygen.

Twitter del.icio.us Digg Facebook linked-in Yahoo Buzz StumbleUpon

Welding gas guards the weld puddle:

Monday, January 3rd, 2011

The reason that you need the shielding gas is so that it can guard the welding arc from oxygen and additional gases in the nearby air close to the welding arc.

Shielding gas comes in a variety of flavors.
Which one you must use all depends on;

1. What type of welding process you are using
2. What quality of welding bead appearance you want
3. What material you are welding
4. Economical choice of gas to use
5. What type of consumable electrode you are using
6. Level of welding penetration required

The majority normally used mig welding wire in Australia by AWS standards is what is called ER70S-6 welding wire. And the most ordinary welding gas that is used with this is a mixed gas of carbon dioxide (CO2) and argon (Ar), at a ratio of 75%Ar to 25%CO2.

This is also called C25 in the USA. (i.e. C for carbon at 25%).Other than you can also use straight carbon dioxide (CO2), or you can use straight Argon (Ar). The CO2 will provide you much deeper welding diffusion, and it is far cheaper to buy as it is not mixed in with other gases. But on the problem the weld beads will not be as smooth as with mixed gas and there will be a lot additional spatter.

Twitter del.icio.us Digg Facebook linked-in Yahoo Buzz StumbleUpon

Gas Welding – Basic Security Precautions:

Thursday, November 25th, 2010

Previous to starting gas welding or cutting take away from the neighborhood any flammable material or everything that might be spoiled by heat or sparks which are often thrown a long distance. Containers which had held combustion able or flammable materials must be welded only after exercising appropriate safety measures.

Fire extinguishers or sand must be available at hand. Don’t weld in restricted spaces without sufficient ventilation or individual respiratory gear. When welding inside boilers or extra restricted spaces, the gas cylinders should be kept outside and the hosepipe and its attachments carefully inspected for leak. Gas flame must not be allowable to play even for a moment on the cylinders or their add-ons. Do not pick up hot jobs or objects.

Use spectacles with nonflammable lenses and frames. Not at all do any chipping or grinding with no appropriate spectacles. Don’t weld painted or galvanized surfaces in a badly ventilated space. Don’t use matches for lighting torches. This may result in hand burns. By no means attempt to renew a blow pipe that has blown out with no first closing both valves and relighting in the correct way.

If welding or cutting is to be stopped up for the moment, release the pressure adjusting screws of the regulators by rotating them to the left. If welding or cutting is to be stopped up for a long time, lock the cylinder valves and then release all gas pressures from the regulators and hosepipe by opening the torch valves for a moment. Close the torch valves and discharge the pressure adjusting screws.