Nothing special here. A fellow brought two bases and two tops, One I had to cut a pipe off of. It is for him to display his metal art. A couple pictures. All MIG with Everlast IMIG-250P with ER70-6, 21 volts and about 200 on the wire-feed speed. Was outside and it was windy, as you can see the spatter.

Round one
Click image for larger version. 

Name:	2013-03-15 16.12.08.jpg 
Views:	315 
Size:	144.5 KB 
ID:	9831
Square one, non cleaned up or painted .
Click image for larger version. 

Name:	2013-03-15 16.56.51.jpg 
Views:	321 
Size:	146.8 KB 
ID:	9833
Penetration, mine is outer one. It had a pipe welder to it same and the squared one.
Click image for larger version. 

Name:	2013-03-15 16.12.20.jpg 
Views:	341 
Size:	134.1 KB 
ID:	9832
Final product.
Click image for larger version. 

Name:	2013-03-16 16.05.59.jpg 
Views:	313 
Size:	151.8 KB 
ID:	9830

Will show the art later, he has us doing the artwork. If he OKs it I will post that too. All polished SS.