    Making the press benders does require knowing some things such as making sure you have the bender guided so that you don't put any side load on the press bar causing it to bend instead of the intended material.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  2. #22

    Default

    Nice video Rambozo ... wish I had his big foot control acuated press.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  3. #23

    Default

    Quote Originally Posted by MuttonHawg View Post
    You're looking for sources of chains? I have a boatload of old bicycle chains, if you were interested in those. I kept them around because I heard of somewhere that would make picture frames and stuff out of them, but I never got around to collecting them all into one box and figuring out where to send them. Or were you looking for something bigger, like automotive timing/sync chains?
    Thanks I do have a good source for bicycle chains but I have more use for ansi 40,50 &60 as well as multi link like timing and primary drive chains. I do ok I seldom have to buy chains unless I have a call for something special where there is a load requirement and I need new chain.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  4. #24

    Default

    I've decided to piece together my own press break … it won’t be as slick as the one in the kit that Swagoffroad.com puts out but I think it will cost a heck of a lot less … I figure it will take about $15 to $20 worth of steel. Gas, electricity and rod ( or wire) to complete.
    BTW I shortened the video of the “Winky dinky metal bender” and replaced the old one on youtube with it. It really wasn’t intended to be a tutorial … just another chance to look at sparks and plug my music hehehe … yes, I realize my sound is too tame for the younger folks but … never say die(yes, I know tame rhymes with lame ... let's not go there ok?) … lmao http://youtu.be/1bR-2HyAqDo
    Last edited by Winky; 01-25-2013 at 01:09 PM.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  5. #25

    Default

    I bit the bullet and got one of the Swag press brake kits w/o the back stop ... was a breeze to build ... of course I had to make a video yes I used mig ... I've reserving my tig set up for aluminum, SS and thin sheet metal ... I will start using it for more DCEN on mild steel again soon. http://youtu.be/ocZwDXVfs4s
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  6. #26

    Default

    Quote Originally Posted by Winky View Post
    I bit the bullet and got one of the Swag press brake kits w/o the back stop ... was a breeze to build ... of course I had to make a video yes I used mig ... I've reserving my tig set up for aluminum, SS and thin sheet metal ... I will start using it for more DCEN on mild steel again soon. http://youtu.be/ocZwDXVfs4s
    I just bought the 20 ton HD with no backstop, sould be here this week.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #27

    Default

    Quote Originally Posted by zoama585 View Post
    I just bought the 20 ton HD with no backstop, sould be here this week.
    You'll like it ... just remember to weld the bottom die in steps to avoid warping and make sure you square the guide posts ... it only took me around 35 to 40 minutes to put mine together ... works great too!
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  8. #28

    Default

    I could show this as a project to give me an additional entry but I'm not going to ... I'll have at least four as it is ... by the way I know what I'll get if I win the big green bucks a ... 205P mig unit ... sweet looking machine, I can use it ... onto to my post I've just made another set of window bars for a different window on the house (already have the shop covered)Click image for larger version. 

Name:	window bars 2 unfinished.jpg 
Views:	352 
Size:	129.9 KB 
ID:	9351Click image for larger version. 

Name:	front window bars with spider.jpg 
Views:	363 
Size:	143.4 KB 
ID:	9352 Have a great day my friends!
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  9. #29

    Default

    Quote Originally Posted by Winky View Post
    I could show this as a project to give me an additional entry but I'm not going to ... I'll have at least four as it is ... by the way I know what I'll get if I win the big green bucks a ... 205P mig unit ... sweet looking machine, I can use it ... onto to my post I've just made another set of window bars for a different window on the house (already have the shop covered)Click image for larger version. 

Name:	window bars 2 unfinished.jpg 
Views:	352 
Size:	129.9 KB 
ID:	9351Click image for larger version. 

Name:	front window bars with spider.jpg 
Views:	363 
Size:	143.4 KB 
ID:	9352 Have a great day my friends!
    Actually I thought about it and since I made these bar sets during the contest it doesn't make any sense not to include them as entries SO I'm going to enter both sets of bars that I made as ... PROJECT # 3 Home and Shop Security here are some pictures of the other bar sets that I made ... if I can do it this way without starting a thread ... I'll go back and look at the rules again but for now ... Click image for larger version. 

Name:	fleur-de-lis 1.jpg 
Views:	345 
Size:	126.5 KB 
ID:	9369Click image for larger version. 

Name:	window dressing.jpg 
Views:	370 
Size:	116.0 KB 
ID:	9370Click image for larger version. 

Name:	security window bars with mounts.jpg 
Views:	354 
Size:	122.6 KB 
ID:	9371 I couldn't find mention if each project needed to have it's own thread or not ... I wish there was a way to edit threads ... aagghh this computer stuff makes me crazy sometimes ... I'm so confused lmao.
    Last edited by Winky; 02-10-2013 at 10:01 AM.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

Similar Threads

  1. Project 1 from EmptyNester. Category: Custom Shop Tools - CNC Table
    By EmptyNester in forum Other Custom Fabrications
    Replies: 116
    Last Post: 03-10-2013, 11:27 PM
  2. Project 1 from Winky. Category: metal art
    By Winky in forum Metal Art
    Replies: 2
    Last Post: 02-12-2013, 12:54 PM
  3. Project 3 from Winky. Category: Home and Shop Security
    By Winky in forum Other Custom Fabrications
    Replies: 0
    Last Post: 02-11-2013, 12:09 PM
  4. Replies: 6
    Last Post: 01-03-2013, 11:54 AM
  5. Project 3 from KSmith. Category: Custom Shop Tools – Band Saw Stand
    By KSmith in forum Other Custom Fabrications
    Replies: 1
    Last Post: 09-25-2012, 07:32 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •