    Arrow Project 1 from Rambozo. Category: Custom Automotive Off Road Welding

    I've been meaning to post this project, I actually finished it before my 140ST came, so no Everlast on this. It does have MIG, TIG, and SMAW just because of the situation or what would work best. The TIG was mostly my CyberTIG, the stick was a Miller Thunderbolt, and the MIG was a Century 120 volt mostly used for tacking.
    This is going to be a tractor mounted weed sprayer. Started from the bottom with the skids. Cut up some square tube for them, and TIG welded them up. Smoothed the sides a little. Because my original plan called for a lot more 45° joints, I made up a 22.5° square to check parts and set the saw. Then started on the upper cage parts. The lower rails are 3" channel and I welded them and the skids with stick.

    Click image for larger version. 

Name:	Projects 618.JPG 
Views:	1054 
Size:	90.7 KB 
ID:	8061 Click image for larger version. 

Name:	Projects 623.JPG 
Views:	1017 
Size:	96.4 KB 
ID:	8062 Click image for larger version. 

Name:	Projects 627.JPG 
Views:	963 
Size:	79.2 KB 
ID:	8063 Click image for larger version. 

Name:	Projects 633.JPG 
Views:	1021 
Size:	84.4 KB 
ID:	8064 Click image for larger version. 

Name:	Projects 634.JPG 
Views:	1006 
Size:	72.1 KB 
ID:	8065

    Here is the finished frame attached to the tractor, then lifted on the 3 point. The mounts keep it level at all times. The tank is recycled from another sprayer, it's 100 gallons. Then I added mounts for the equipment, and gave it some paint. The customer likes everything done in white for some reason. Wouldn't be my first choice for somthing like this.

    Click image for larger version. 

Name:	Projects 637.JPG 
Views:	981 
Size:	70.7 KB 
ID:	8066 Click image for larger version. 

Name:	Projects 640.JPG 
Views:	995 
Size:	80.4 KB 
ID:	8067 Click image for larger version. 

Name:	Projects 642.JPG 
Views:	1010 
Size:	71.8 KB 
ID:	8068 Click image for larger version. 

Name:	Projects 645.JPG 
Views:	1013 
Size:	61.2 KB 
ID:	8069
    Last edited by Rambozo; 09-28-2012 at 01:36 AM.
    Long arc, short arc, heliarc and in-the-dark!

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Here it is all assembled and installed. I added a pressure guage and a couple of switches to the tractor. The PTO pump was recycled from yet another sprayer project and setup with camlock fittings. There are two motorized ball valves that control two boomless spray nozzles. They spray about 20' to each side for a 40' total swath. The strainer is accessable through the gap above the skids, and there is an air gap setup for filling the tank, also with a camlock for the hose. The electrics connect with a twist lock plug and a quick release hose fitting for the pressure guage. The pressure is controlled by engine RPM and there is a small manual bypass valve to operate a jet agitation system inside the tank.

    Click image for larger version. 

Name:	Projects 676.JPG 
Views:	946 
Size:	59.8 KB 
ID:	8071 Click image for larger version. 

Name:	Projects 678.JPG 
Views:	986 
Size:	75.3 KB 
ID:	8073 Click image for larger version. 

Name:	Projects 680.JPG 
Views:	966 
Size:	91.2 KB 
ID:	8074 Click image for larger version. 

Name:	Projects 681.JPG 
Views:	929 
Size:	52.1 KB 
ID:	8075 Click image for larger version. 

Name:	Projects 684.JPG 
Views:	955 
Size:	33.6 KB 
ID:	8076 Click image for larger version. 

Name:	Projects 690.JPG 
Views:	910 
Size:	60.2 KB 
ID:	8077 Click image for larger version. 

Name:	Projects 691.JPG 
Views:	974 
Size:	57.1 KB 
ID:	8072
    Long arc, short arc, heliarc and in-the-dark!

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Next up was some add on for hand spraying. More miter cuts. If I did this a lot I would get a few saws so I could leave them set at different angles. Tacked things up and checked the fit. This is going to hold this reel using the mounting for the front weights. Another TIG job. Welded up and fits fine. Paint and install. Since the tractor frame is gray I went with that instead of more aweful white.

    Click image for larger version. 

Name:	Projects 692.JPG 
Views:	968 
Size:	73.4 KB 
ID:	8079 Click image for larger version. 

Name:	Projects 697.JPG 
Views:	988 
Size:	92.2 KB 
ID:	8081 Click image for larger version. 

Name:	Projects 696.JPG 
Views:	938 
Size:	87.2 KB 
ID:	8080 Click image for larger version. 

Name:	Projects 701.JPG 
Views:	947 
Size:	56.3 KB 
ID:	8082 Click image for larger version. 

Name:	Projects 708.JPG 
Views:	943 
Size:	88.1 KB 
ID:	8083 Click image for larger version. 

Name:	Projects 710.JPG 
Views:	1002 
Size:	95.5 KB 
ID:	8084 Click image for larger version. 

Name:	Projects 711.JPG 
Views:	964 
Size:	89.8 KB 
ID:	8085 Click image for larger version. 

Name:	Projects 717.JPG 
Views:	952 
Size:	73.5 KB 
ID:	8086

    And lastly another recycled spray gun holder cut off something and welded to a new mounting to go where some stock handle was on the fender.

    Click image for larger version. 

Name:	Projects 719.JPG 
Views:	959 
Size:	85.2 KB 
ID:	8087 Click image for larger version. 

Name:	Projects 721.JPG 
Views:	932 
Size:	31.5 KB 
ID:	8078

    And because I was trying to explain something to someone, I shot a video of my oddball unconventional stick technique. I don't always do this, but it works for me to be steady with a full length electrode and no place to prop or if I can't use both hands. I just hold the electrode, and let the stinger rest on the back of my hand.

    Long arc, short arc, heliarc and in-the-dark!

  4. #4
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Cool project! I like your unconventional stick welding technique. I've wondered what other people do to steady the rod when it is fresh. Especially the longer rods. I'm not sure I'll be doing that myself but it sure was interesting to watch!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I know Jody at WT&T breaks off the flux to shorten the rod, but I guess I'm too cheap to waste rods like that.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rambozo View Post
    I know Jody at WT&T breaks off the flux to shorten the rod, but I guess I'm too cheap to waste rods like that.
    I saw that video. You aren't alone. LOL I'd be trying your technique before I resort to losing a bit of rod. Shoot, I burn 'em right down to the nub ....
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  7. #7
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Nice work as usual- what did you use for the mitre cuts? I'm looking forward to viewing the stick technique video (can't run it at work). Any concerns about the weight of a full tank upsetting the balance of the tractor? The hose reel up front would offset that some, but it's a sizeable looking tank.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  8. #8
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by DaveO View Post
    Nice work as usual- what did you use for the mitre cuts? I'm looking forward to viewing the stick technique video (can't run it at work). Any concerns about the weight of a full tank upsetting the balance of the tractor? The hose reel up front would offset that some, but it's a sizeable looking tank.
    Click image for larger version. 

Name:	Projects 710.JPG 
Views:	1002 
Size:	95.5 KB 
ID:	8084

    That is quite a stack of suitcase weights there, if that doesn't keep it from popping wheelies I don't know what will!
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  9. #9
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    My bad, don't know how I could have missed those photos.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by DaveO View Post
    Nice work as usual- what did you use for the mitre cuts? I'm looking forward to viewing the stick technique video (can't run it at work). Any concerns about the weight of a full tank upsetting the balance of the tractor? The hose reel up front would offset that some, but it's a sizeable looking tank.
    I used an abrasive chop saw. Someday I would like to get one of the carbide saws as I hate the grit spewed out by the abrasive blade, and the parts being hot.
    Weight was one of the main reasons for building this instead of buying a commercial product. I kept the tank about as close to the 3 point as I could. Most of the commercial units hang much farther back. Now that it has been used a bunch, they ended up taking off two of the suitcase weights and it still handles just fine. I worked out that I could have probably used a 150 gallon tank, but this one was on hand.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Project 2 from Rambozo. Category: Automotive On Road Trailer Jack
    By Rambozo in forum Other Custom Fabrications
    Replies: 5
    Last Post: 07-01-2015, 07:56 AM
  2. Replies: 10
    Last Post: 02-19-2013, 01:26 PM
  3. Replies: 28
    Last Post: 12-10-2012, 12:21 AM
  4. Project 2 from Undercut. Category: Custom Automotive
    By undercut in forum Other Custom Fabrications
    Replies: 8
    Last Post: 10-03-2012, 10:38 PM
  5. Project 1 from Hooda. Category: 3) Custom Automotive on/off road Welding.
    By hooda in forum Personal Projects (no welder required)
    Replies: 8
    Last Post: 04-03-2012, 04:05 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •