I wanted to try out my new Plasma cutter so I decided to cut some flames.
After a little more thought, I decided to make a shelf for my garage with a flame back piece.
I used some Aluminum sheet I had left over from a job, I'm think it is .094 thickness.
I used my PP50 plasma cutter and my EX250 TIG to weld it.
I found out that flames are not as easy to draw as I thought.
I spent probably an hour drawing and wiping off different flames till I finally settled with what I have.
Straight edge for Plasma cutting...
Drill holes...
Clamp down the thick bar stock to bend the sides and front...
cut flames....
Weld up and use tool box liner for the bottom of the shelf!
![]()












Reply With Quote