Share
Page 2 of 2 FirstFirst 12
Results 21 to 34 of 34

Thread: PP50 wont make second cut with out first turning machine off and on

  1. #21

    Default

    It's in the machine in line with the air inlet and looks like a solenoid (how do you describe a solenoid? you know it when you see it sort of thing..)....with wires going to it...

  2. #22

    Default

    Inline at the back of the machine is most welders. And a hose in (from the back of the machine) and hose out and wires going to it. Like Mark said you will know it when you see it. The TIG ones have a around top square base and 4 corner screws.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #23
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by trickbiker View Post
    Where is the solenoid valve and what does it look like? Mickey
    Follow the hose, it always knows.
    Long arc, short arc, heliarc and in-the-dark!

  4. #24

    Default

    Thanks Mike, I have been agravatingly useing it all day today but I want to open it up tomorrow and check out what sas been described to me. "Will get back when either I've brocken it worse or fixed it. Thanks Mickey
    Trickbiker

  5. #25

    Default

    Ok, found a picture of "a" solenoid from a proto model I had we never introduced. Looks similar...not exactly though and it is on the other side IF I remember right or it hasn't been changed.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	20100823_82.jpg 
Views:	315 
Size:	138.6 KB 
ID:	9165  

  6. #26

    Default

    Thank you so much. Working on it in a few minutes
    Trickbiker

  7. Default

    Here is the actual solenoid you will be looking for.
    Cheers
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	image.jpg 
Views:	333 
Size:	132.4 KB 
ID:	9173  
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  8. #28

    Default

    I just came in from opening it up adn pulling the solenoid out. I streght the spring and cleaned the slyd. Then I put some molitheum grease on it and then wiped it off leaveing a slight filml. Put it back together and, nada, did the same thing, all air and not flame untill I turn the unit off. ?
    Trickbiker

  9. #29

    Default

    Grease is too heavy...way too heavy...Even a light film. It will make it stick for sure.
    How much post flow time are you using?

  10. #30

    Default

    Mark I'm using no post time. A lot times if I unscrew the head pieces the air will quit. But normally I have to turn the machine off and on again. I can't cut expanded metal anymore.
    Trickbiker

  11. #31

    Default

    The pilot arc isn't relighting? Can you have someone help you and see if the hear or feel a click when you let go of the switch? Just feel of the case or listen closely. If you do, that is the relay that is controlling the solenoid..and should be working...then its an issue with the solenoid. If you can't hear it,it doesn't mean it isn't working, but that it just may be a soft release. I think you'll be able to hear it if you listen closely. Its on the top board, a black or gray little box. You can call in and talk with Ray at ext 207 if you need to. And he can go through some things with you.

  12. #32

    Default

    Thanks, I'll have it apart when I call him. Thats right, after the cut the pilot arc will not come on untill the air stops either by me unscrewing the tip or shutting the machine off.The top board is not secured real good. When I took the cover off I saw it moveing a lot and one stand off was not attached. Thanks again. Mickey
    Trickbiker

  13. #33

    Default

    Mickey, before you open it, unscrew the torch (or torch control depending on model) but leave it plugged in, fire the torch and let off. While the air is stuck on, unplug the torch/torch control and see if the air flow stops. I had a loose wire in the torch do that once.

    But sounds like solenoid or relay.

    And grease is too thick for it.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  14. #34

    Default

    Thanks Mike and other contributers BUT, must have scared it because after pulling the selinod out and cleaning it with no change, the next day with the idea you gave of Calling Alex it starting working without any hesitation. Thanks again for all the replys, it was really bugging me.
    Trickbiker

Similar Threads

  1. New diy cnc machine pp50 with thc
    By waynagen in forum Everlast Plasma Cutters (PAC)
    Replies: 17
    Last Post: 01-13-2014, 01:14 PM
  2. HF when turning on PT 200 DX
    By willida in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 01-26-2013, 04:49 PM
  3. Torch wont arc
    By Fomdiddle in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 09-07-2011, 11:53 PM
  4. Engine turning
    By Ram48 in forum Personal Projects (no welder required)
    Replies: 7
    Last Post: 06-07-2011, 12:53 AM
  5. 250 ex arc wont start
    By johnson697 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 05-26-2010, 03:40 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •