  1. #21

    Default

    The roll is actually 44 lbs.
    What most people don't know is that frequently the price that they are quoted on other wire, while the same diameter roll, is only 30 lbs. But when you get 14 MORE pounds on a roll, the price goes up.

  2. #22

    Default

    Quote Originally Posted by performance View Post
    The roll is actually 44 lbs.
    What most people don't know is that frequently the price that they are quoted on other wire, while the same diameter roll, is only 30 lbs. But when you get 14 MORE pounds on a roll, the price goes up.
    I bought a roll from the ebay guy... says 40 lb 18kg on the box. The lws said the same, 40 lb. Click image for larger version. 

Name:	12.50.jpg 
Views:	541 
Size:	36.1 KB 
ID:	7433
    It's a high price but I gotta see for myself how it does.
    Last edited by zoama; 07-25-2012 at 12:03 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #23

    Default

    I hope that wire isn't rusty. The box is suspect.

  4. #24

    Default

    Quote Originally Posted by performance View Post
    I hope that wire isn't rusty. The box is suspect.
    The wire I use is copper coated... Or it looks that way... I was told it was to keep it from rusting. I know raw steel will rust in seconds in a humid environment. I live in a humid area and never had a problem with rusty wire.

    Isn't all MIG wire coated like that???
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  5. #25

    Default

    Quote Originally Posted by Brian Ski View Post
    The wire I use is copper coated... Or it looks that way... I was told it was to keep it from rusting. I know raw steel will rust in seconds in a humid environment. I live in a humid area and never had a problem with rusty wire.

    Isn't all MIG wire coated like that???
    http://products.esabna.com/EN/home/f...od_1250_er70s6
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #26

    Default

    Quote Originally Posted by Brian Ski View Post
    The wire I use is copper coated... Or it looks that way... I was told it was to keep it from rusting. I know raw steel will rust in seconds in a humid environment. I live in a humid area and never had a problem with rusty wire.

    Isn't all MIG wire coated like that???
    The cheap stuff usually is. Copper is used as a substitute deoxidizer, but it also can add impurity to the weld. Plus you end up with the problem of the copper flaking and packing your gun liner and can cause drive roll issues long term.

    Edit: Lookie what I just found:
    Things that make you go hmmm. That OK 12.50 sounds better by the moment, doesn't it? You won't find a cheap copper wire that isn't coated, or at least I haven't seen it. The national standard wire that I talked about isn't coated either.

    http://www.esabna.com/ca/en/Products/OK-Autrod-1250.cfm
    Last edited by performance; 07-25-2012 at 04:44 AM.

  7. #27

    Default

    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #28

    Default

    Quote Originally Posted by zoama585 View Post
    very cool video
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  9. #29

    Default

    Quote Originally Posted by performance View Post
    The cheap stuff usually is. Copper is used as a substitute deoxidizer, but it also can add impurity to the weld. Plus you end up with the problem of the copper flaking and packing your gun liner and can cause drive roll issues long term.

    Edit: Lookie what I just found:
    Things that make you go hmmm. That OK 12.50 sounds better by the moment, doesn't it? You won't find a cheap copper wire that isn't coated, or at least I haven't seen it. The national standard wire that I talked about isn't coated either.

    http://www.esabna.com/ca/en/Products/OK-Autrod-1250.cfm
    I notice that stuff it blue... I don't see where it says if it is coated... Maybe not??? Looks like a lot better wire. But for the long term between uses is there is a rust or corrosion problem sounds like not for me. Sometimes I can go for several rolls a year and other times a roll can last several years. With the humidity here I can see surface rust forming on tools if I leave the garage door open on a damp day.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  10. #30

    Default

    Brian, it is not coated with copper, but that does not mean it will rust any faster than copper coated wire. I've had copper wire rust on me faster than this stuff. Copper wire will rust. As far as not using it, and the wire rusting, IF a wire does oxidize, it is usually only the top layer of wire, and once that is removed, the wire beneath is just fine, if it is on a closed spool. I live in S. GA, 2 hours from the gulf, and 2 hours from the Atlantic. It doesn't get much more humid, with summer averages around 80-90% humidity.

  11. #31

    Default

    Mark... Thanks for the info... Learning all the time. Will have to cut off a few pieces of wire and see how they hold up to rusting. Looks like the Esab wire is protected/sealed somehow.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  12. #32

    Default

    The ebay guy still hasn't shipped. I asked him to put a hard backer on each side of the spool in hopes of avoiding shipping damage.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  13. #33

    Default

    i keep my mig wire from rusting is i spray anti spatter spray on my wire spools i store . . when i get done welding i open my side cover and spray the outside of spool with anti spatter spray works good
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  14. #34

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    i keep my mig wire from rusting is i spray anti spatter spray on my wire spools i store . . when i get done welding i open my side cover and spray the outside of spool with anti spatter spray works good
    Isn't anti-spatter spray just soapy water ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  15. #35

    Default

    Click image for larger version. 

Name:	37030.jpg 
Views:	562 
Size:	8.8 KB 
ID:	7436No its can be silicone or DICHLOROMETHANE . the good anti spatter spray is made with DICHLOROMETHANE methylene chloride i use this spray works awesome for keep mig tip clean
    Last edited by Rodsmachineshop; 07-26-2012 at 03:05 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  16. #36

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    No its can be silicone or DICHLOROMETHANE . the good anti spatter spray is made with DICHLOROMETHANE methylene chloride i use this spray works awesome for keep mig tip clean
    I've got a can of hobart brand... looks like windex to me.

    Edit: http://en.wikipedia.org/wiki/Dichloromethane Looks like some nasty stuff.
    Last edited by zoama; 07-26-2012 at 03:14 AM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  17. #37

    Default

    I have used the Hobart don't work very well cant even find a MSDS for it so is probably Windex lol check out msds on what is used for food prossessing they use lye and other bad stuff
    Last edited by Rodsmachineshop; 07-26-2012 at 03:40 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  18. #38

    Default

    The anti spatter the guys use at work is some sort of fish oil base I believe. Smells like Long John Silvers when it is being used. Not sure of the brand but it is a red and silver can.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  19. #39
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Another take on the oil based products.
    http://www.weldingtipsandtricks.com/...ng-tip-20.html
    Long arc, short arc, heliarc and in-the-dark!

  20. #40

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    Click image for larger version. 

Name:	37030.jpg 
Views:	562 
Size:	8.8 KB 
ID:	7436No its can be silicone or DICHLOROMETHANE . the good anti spatter spray is made with DICHLOROMETHANE methylene chloride i use this spray works awesome for keep mig tip clean
    The only problem with that is that it will cause impurities and porosity in your weld. When that stuff is heated up it goes to gas, and when it does it creates air bubbles beneath the surface of the weld. Only a little should be used inside the gun nozzle and non weld areas.

Similar Threads

  1. PowerPro 256 makes HF but wont start arc
    By acannell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 06-25-2016, 06:03 AM
  2. What makes PP 60C ideal for CNC?
    By RichardH in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 01-06-2014, 04:25 PM
  3. Powerpro 205 makes me think one day i can call myself a welder
    By Chuck_jkl in forum Customer Testimonials
    Replies: 6
    Last Post: 02-01-2013, 01:05 AM
  4. Replies: 26
    Last Post: 02-22-2012, 11:25 AM
  5. Anyone who makes Aluminum catch cans or reservoirs...Question?
    By CGCINC in forum General Welding Questions
    Replies: 9
    Last Post: 12-08-2011, 01:38 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •