Who makes the best ER70S-6 mig wire ?
Is there a difference in quality between manufacturers ?
Where do you buy ?
Who makes the best ER70S-6 mig wire ?
Is there a difference in quality between manufacturers ?
Where do you buy ?
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.
I guess I have not compared... But I usually get mine from Harbor Freight... It used to be if you broke $50 you would get free shipping... Plus there is a store nearby. They do stock it here...
http://www.harborfreight.com/0030-in...oll-42919.html
Shade tree MIG welder.
I buy cheap wire!!! but yes there is a difference and I know people who will only buy Lincoln wire. Lately I have been using Radnor wire and have had good luck, but I have read were people had problems. I have also used some inweld mig wire and tig rods with good luck.
A guy in my town has a machine/welding shop and bought a roll of cheap mig wire because a salesman told him it was good stuff. All of the sudden his machine started going nuts; he would weld and the machine would start sputtering and then clear out and run smooth. It continued over and over again and he thought something was wrong with his welder. He bought a new liner for his gun, new drive wheels, and it still did the same thing again and again. He finally unrolled 4-5 feet of wire and it had some some places where the wire was thicker than .045. He unrolled another 4-5 feet of wire and checked it as well and the same thing again. I have heard other people having similar problems. From what the guy told me he unrolled 25-30 feet of lincoln wire and checked it as well; he said it measured correct with no variances.
Everlast Power Arc 200 --> Money Maker$$
Everlast Power Arc 140ST
Everlast IMig 200
Everlast Power Tig 225lx
Everlast Power Super Cut 50
Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
Everlast PowerTig 200DX - Sold! Fantastic Machine!
Victor cutting torch
HF 20 Ton Shop Press
HF 4x6 Band Saw
HF Air Compressor
Northern Tool Drill Press
Powerhouse 7000 watt generator
www.murphywelding.com
National makes a GOOD wire.
But the best?
ESAB OK Aristorod 12.50
Without a shadow of a doubt.
For a decent cheapy...Techniweld.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
I'll never buy HF wire again. I buy Lincoln and Hobart at the lowest end. Chicago Electric was the worst wire I ever bought, so bad I stopped welding and pulled it from the machine. Bad arc, breaks, jams, crappy weld quality, etc.
Trip Bauer
Former USN HT
Everlast 200DX New Model
Hobart Handler 125 MIG
Van Norman #12
Atlas 12" engine lathe
'98 RoadKing - 84 Ironhead - 59 Ironhead
Maybe next time I will have to give another kind a try... Hate to say it out loud... But I have never had a break or jam with their wire. I have used miles of it. As far as quality... Hard to say a lot of the stuff I use it on is rusty and dirty. Almost always used for fixing rather than projects.
Shade tree MIG welder.
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.
I have good results with Harris ER70S-6 and if you compare the detailed specifications with Lincoln, Hobart, Radnor, Victor etc they're all identical in composition.
PowerTig 250EXT ordered on 2/20/12 - AluMig~250P - MasterTig~250AC - Matco Mig~Spot Welder - Giaintec CAT250D - Harris Steelworker Oxy/Acet - Henrob DHC 2000 - Van Norman CB1401 - Lagun FTV1 Mill - CM Mill/Drill - CM 13x40 Lathe - CM 7x12 Bandsaw - CM 6x48 Belt Sander - CM 12 Disc Sander - Baldor 3/4HP Buffer - TP 960 Blast Cab - 48~Box & Pan Break - 52~Foot Shear - 20~Ton Press - 80~Gal 7.5HP Compressor - 9' Snap On Tool Box - 30' Stainless Tool Box Workbench - 3M Speedglas 9100Xx
Maybe these welders are tuned with Aristrorod, it's the one ESAB product that is made in China.
It's funny, where I used to work we had an ESAB that ran best on Hobart wire, and a Hobart that was best with ESAB SpoolArc 86. The machines were used for different jobs, but I always thought that was odd. If you swapped wires, neither machine worked as well. I was told at the time it had to do with the inductance of the machines as these did not have all the bells and whistles of modern MIG welders.
Long arc, short arc, heliarc and in-the-dark!
I use any wire that's the cheapest , to me they weld all the same to me if i adjust gas flow , some need more gas flow and some need less . most the time i use forney mig wire , since best price were i live
Last edited by Rodsmachineshop; 07-21-2012 at 03:04 AM.
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.
You can usually buy it through your local distributor. It is worth every cent trust me. Don't give up on it. Try the national brand next though if you just can't find it or order it through your lws.
Praxiar, Wescoweld.com
Last edited by performance; 07-21-2012 at 03:57 AM.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Hahaha.... Right after you said you would try it, I thought I would look into it... I found a 20 or 40Lb box of it on ebay and nothing else. I thought I would wait and see what you posted where you got it from. I can find listings for it but no retailers... At least in my limited looking. Was curious what the price is. If it is a little higher or extremely expensive.
Shade tree MIG welder.
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.
It's about 80.00 per roll locally with shipping (if it has to be special ordered). It's a 44lb roll. With reduced spatter, and less pre weld cleanup and all factor's considered, it isn't bad at all. Again, it's worth it to me.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.
I have to agree with you Rod,,,but there are differences in the metal in the wire, depending on the maker,,,which takes me back to my early days in the oldmans body shop,,if you had an American car and an import with the paint on the fenders ground off,,and left them over night or over the weekend,,,in the morning the import would have a yellowish tinge of oxidation on the exposed metal,,,likely due to the absense of chome in the recycled metal used to build them,,,today everything is recycled metal and that can affect the heat required to melt it or the gas required to protect it,,,So each maker of wire makes it to the spec,, but there are subtle differences..most important thing is to get properly packaged and stored wire,,,,rusty wire from a good maker is stil crap..
Some of those lies people tell about me, are true
Always been happy with Lincoln SuperArc 70S6 for mild steel. S/F....Ken M
Lincoln Power MIG 300
Everlast 160STH
Miller 225 Thunderbolt (sold it)
Lincoln Squarewave 175 TIG(traded it for)
Miller DEL 200 welder/genset
Thermal Dynamics 1250XL plasma cutter
Miller XMT300
My lws wants $100=shipping for a 40LB roll... I told them NO.
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.