Thread: Imig250p (pulse explained)

  1. Default Imig250p (pulse explained)

    Hello,

    I have been reading about your pulse and similar units. Your manual nor any posts explains how your pulse works and what each knob does. I know your unit is not a Synergic mig pulse so I am totally confused. From what i can deduce (pardon if im wrong). Is that its not really a pulse but more of spot/stitch control?
    Is pulse voltage spot welding and stitch welding base voltage etc etc? If not please explain as its conusing.

    Regards and thanks in advance

  2. #2

    Default

    No it's a pulse. Spot stitch is something completely different.

    Just as with any pulse you have your pulse width (time on) and frequency controls.
    Instead of pulsing amps, you are pulsing volts with MIG between to levels rapidly at a minimum of 20 hz up to 200 hz.
    The pulse time on adjusts the time spent in the high voltage part of the pulse verses the low voltage part.

    This is designed to pulse rapidly between spray and globular transfer, allowing the voltage to dip briefly down into the globular range long enough to cool off but desposit little if any metal. This in theory allows you to weld out of position with the unit.

    The "synergic" mig is preprogrammed with various settings of the pulse width and frequency for any given setting. All it does is take away some of the science behind the pulse and give the operator a preset point of operation. Most of these migs have background menus that allow manual setting of the pulse as well, as in the Miller 350P.

  3. Default

    To use the pulse dont you use a different gas from the 75/25. Is pulse only used in spray transfer?
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  4. #4

    Default

    Ideally? Yes. I use a little different blend for spray than many folks, but it works well with my ESAB. I use a C-18. Less than 20% CO2 is all that is really required with many welders, and is the technical limit. The c-18 still allows useful welding with non spray as well. In fact it is downright nice.

  5. #5
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Pulse welding aluminum with a spool gun with the I mig 250P or 205P using 75%/25% Helium Argon has any one tried it, I was thing of get the 250P or 205P if it works other welders with pulse are double pulse not single pulse like the Everlast Mig Pulse.

  6. #6

    Default

    Kempy, your post is a little confusing. Can you try to retype it?

  7. #7
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by Kempy View Post
    Pulse welding aluminum with a spool gun with the I mig 250P or 205P using 75%/25% Helium Argon has any one tried it, I was thing of get the 250P or 205P if it works other welders with pulse are double pulse not single pulse like the Everlast Mig Pulse.
    Is any one using a spool gun on aluminum using a I mig 205P in pulse mode and how well does it work look at buying one, sorrry the 250P does not have a spool gun connection. The gas can be Argon or Argon Helium mix.
    The Everlast 205P works in single pulse and most of the welders that are on the market are double pulse. If not does it work well with the pulse off.

  8. #8

    Default

    Quote Originally Posted by Kempy View Post
    Is any one using a spool gun on aluminum using a I mig 205P in pulse mode and how well does it work ? I'm looking at buying one... sorrry the 250P does not have a spool gun connection. The gas can be Argon or Argon Helium mix.
    The Everlast 205P works in single pulse and most of the welders that are on the market are double pulse. If not does it work well with the pulse off.
    The 250p does have a spool gun connection but I've never used it. Click image for larger version. 

Name:	sg.jpg 
Views:	418 
Size:	61.8 KB 
ID:	8227
    Last edited by zoama; 10-20-2012 at 04:56 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by zoama585 View Post
    The 250p does have a spool gun connection but I've never used it. Click image for larger version. 

Name:	sg.jpg 
Views:	418 
Size:	61.8 KB 
ID:	8227
    The 250P in Canada do not have it spool gun is a Options as in their flyer. (spool gun ready NO) all the others have them (spool gun ready YES)

  10. #10

    Default

    Canada, doesn't seem to be carrying the models actively in Canada. Not sure why, but that's why they have not updated it. Definitely have fielded quite a few inquiries from up there on the unit.It probably doesn't fit their marketing tactic. We can sell direct in this case. But the 250P's have been relatively trouble free, and it is a good welder.

  11. #11
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by zoama585 View Post
    The 250p does have a spool gun connection but I've never used it. Click image for larger version. 

Name:	sg.jpg 
Views:	418 
Size:	61.8 KB 
ID:	8227
    Ok, that picture brings up another question, how exactly do you switch from DCEP to DCEN?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  12. #12
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I have never seen a Mig machine that switchs - DCEN to + DCEP unless it is a stick SMAW also and then they have Plus + and Neg.- out lets.

  13. #13

    Default

    Quote Originally Posted by redbeard View Post
    Ok, that picture brings up another question, how exactly do you switch from DCEP to DCEN?
    Although not in the first pic I posted, there's a positive and negative dinse connector at the bottom for stick welding. You just connect your leads to the appropriate ones. Click image for larger version. 

Name:	IMG_1233.jpg 
Views:	419 
Size:	138.8 KB 
ID:	8260
    Last edited by zoama; 10-21-2012 at 07:14 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  14. #14
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Kempy View Post
    I have never seen a Mig machine that switchs - DCEN to + DCEP unless it is a stick SMAW also and then they have Plus + and Neg.- out lets.
    I've never seen one that doesn't!

    Most machines have some way to swap polarity as some wires (flux core for one) require DCEN instead of standard DCEP. The online manual for this machine really isn't, it's for the iMIG 200, so there is no description for this machine. Typically there is a terminal block near the drive rollers with jumpers that will let you swap polarity. I'm sure Mike or Mark can provide the details, maybe even a photo.
    Long arc, short arc, heliarc and in-the-dark!

  15. #15

    Default

    Quote Originally Posted by Rambozo View Post
    I've never seen one that doesn't!

    Most machines have some way to swap polarity as some wires (flux core for one) require DCEN instead of standard DCEP. The online manual for this machine really isn't, it's for the iMIG 200, so there is no description for this machine. Typically there is a terminal block near the drive rollers with jumpers that will let you swap polarity. I'm sure Mike or Mark can provide the details, maybe even a photo.
    Quote Originally Posted by zoama585 View Post
    Yep, that's how you swap it for mig.
    Edit: I spoke too soon. I don't see a way to swap polarity inside the cover. Click image for larger version. 

Name:	IMG_1235.jpg 
Views:	452 
Size:	142.7 KB 
ID:	8257Click image for larger version. 

Name:	IMG_1234.jpg 
Views:	432 
Size:	139.8 KB 
ID:	8258Click image for larger version. 

Name:	IMG_1233.jpg 
Views:	456 
Size:	138.8 KB 
ID:	8259
    Last edited by zoama; 10-21-2012 at 07:10 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. Default

    I will let you know soon just got my spool gun in for my 250p I have straight argon, should I be using 75-25 even on smaller aluminum?

  17. #17

    Default

    NEVER use 75/25 when welding aluminum. You can only use PURE argon. And DC+ just like the machine is set up.

    You can change the polarity inside the welder by removing the right cover if I remember right.

  18. Default

    I am referring to argon helium mix, someone said earlier in the post about using a mix gas for aluminum pluse with the spool gun

  19. #19

    Default

    Argon only is perfectly fine. The mixes are more in line with TIG.

  20. Default

    is my 250p supposed to have a - symbol in front of the amperage display the lcd shows -250 is that correct? could the plug be wired wrong, It is not welding good at all, like the polarity is wrong, same with the spoolgun on aluminum tried all kinds of settings and thicknesses and of course all the recommended settings. weld wire on spoolgun and mig gun wants to pile up on surface or go to spray arc and flatten out compleatly

Similar Threads

  1. 255 EXT Help, something went wrong with pulse
    By travis1693 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-20-2018, 10:11 AM
  2. New Everlast Pulse on Pulse Machines?
    By m10za in forum Pre-sales, Sales and Shipping questions
    Replies: 3
    Last Post: 02-04-2015, 07:53 PM
  3. WHo uses Pulse on DC?
    By Johnson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 03-11-2013, 09:17 PM
  4. IMig250P
    By SeanMurphy265 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 05-18-2012, 03:45 AM
  5. Spool Spool / Roll Adaptor for Power IMIg250P, DYI
    By Ray in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 08-10-2010, 07:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •