Code:Gauge 50' 75' 100' 150' 200' #4 100A #3 150A #2 200A 150A 100A #1 250A+ 200A 150A 100A 1/0 350A 250A 200A 125A 100A 2/0 400A+ 300A 250A 150A 100A 3/0 500A 400A 300A 200A 150A 4/0 550A+ 450A+ 350A+ 250A 200A
Code:Gauge 50' 75' 100' 150' 200' #4 100A #3 150A #2 200A 150A 100A #1 250A+ 200A 150A 100A 1/0 350A 250A 200A 125A 100A 2/0 400A+ 300A 250A 150A 100A 3/0 500A 400A 300A 200A 150A 4/0 550A+ 450A+ 350A+ 250A 200A