Been doing a bit of welding on the intake side of a twin turbo setup. Few pics of the progress so far.
![]()
Been doing a bit of welding on the intake side of a twin turbo setup. Few pics of the progress so far.
![]()
Vice Grips
WD-40
Duct Tape
Is this your car? Will this be street legal? Tell us a little about the motor part. I'm guessing to be twin turbo you have to have a stout bottom end?
Everlast Power Arc 200 --> Money Maker$$
Everlast Power Arc 140ST
Everlast IMig 200
Everlast Power Tig 225lx
Everlast Power Super Cut 50
Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
Everlast PowerTig 200DX - Sold! Fantastic Machine!
Victor cutting torch
HF 20 Ton Shop Press
HF 4x6 Band Saw
HF Air Compressor
Northern Tool Drill Press
Powerhouse 7000 watt generator
www.murphywelding.com
Not my car, but potentially street legal, although I doubt it will ever see the street. Motor did right around 800HP N/A and they ran the car that way. Owner immediately decided it was too slow and opted for turbos.
Vice Grips
WD-40
Duct Tape
I can see that, 800 to the wheels is nothing ...Nice welding (and massive snails). I take it you will you be welding all of the tubing to connect everything up? You know you'll need at least a few people to test drive to ensure everything is in order before handing it back to the owner, don't you?
![]()
Is it OK to want to break something just so that you can weld it back together?
Everlast PowerTIG 185 Micro IGBT AC/DC Welder
Everlast Power Arc 200 --> Money Maker$$
Everlast Power Arc 140ST
Everlast IMig 200
Everlast Power Tig 225lx
Everlast Power Super Cut 50
Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
Everlast PowerTig 200DX - Sold! Fantastic Machine!
Victor cutting torch
HF 20 Ton Shop Press
HF 4x6 Band Saw
HF Air Compressor
Northern Tool Drill Press
Powerhouse 7000 watt generator
www.murphywelding.com
are you running inner coolers , coolers are what get the most out of a turbo or supercharger . lol i am a supercharge person so much easier to set up
Last edited by Rodsmachineshop; 05-25-2012 at 04:56 PM.
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
It did 10.0's on just the motor. I have no clue how much it will make after it's all said and done. Depends a lot on how much boost that motor will take. Maybe we'll get a chance to put it on a chassis dyno sometime.
It has water to air intercoolers in the dash, which is why the piping is running from the turbo back through the firewall. Then, after the intercoolers, it will come right out of the firewall and hit the throttle body and intake elbow.
Vice Grips
WD-40
Duct Tape
what engine compression are you running
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list
You can pretty much make as much HP as you want with either single or twin turbos.
My bike is only about 160rwhp stock, and 480rwhp with a single turbo. Only limits are really at the extremes (over 2000HP applications) just due to the physical size of the compressors required.
John
Everlast 200DX
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.95, 154mph 1/8th mile 7.49, 194.27mph 1/4 mile
Welds look good!
And those are some big snails... Definitely looks like a drag car with all that weight up front and water to air IC's in the dash.![]()
"Engineering is the art of modelling materials we do not wholly understand, into shapes we cannot precisely analyze so as to withstand forces we cannot properly assess, in such a way that the public has no reason to suspect the extent of our ignorance."
- Dr. AR Dykes
I like the tubing routing. I definitely wish I had gone out of the engine compartment on my Mustang.
Everlast Powertig 200DX
Miller Synchrowave 200
Miller Dynasty 300 (Work Machine)
Hobart Handler 210MVP
HTP Microcut 30
It is a hayabusa.
You could probably run a completely stock 1000 to low to mid 200's. I don't really have alot of experience with the liter bikes, and even less with street applications for liter bikes.
If you build the bottom ends, over 500hp is possible with the liter bikes as well.
Everlast 200DX
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.95, 154mph 1/8th mile 7.49, 194.27mph 1/4 mile
PowerTig 250EX
Power I-MIG 200
Power Plasma 50
It's what you learn After you know it all that counts!
Any recent updates on this Mustang twin turbo project?
Chris
Everlast Powertig 200DX
Miller Synchrowave 200
Miller Dynasty 300 (Work Machine)
Hobart Handler 210MVP
HTP Microcut 30
Not to dereail the thread, but I'd like to hear more details about the turbo busa. Is there a thread on it? S/F.....Ken M
Lincoln Power MIG 300
Everlast 160STH
Miller 225 Thunderbolt (sold it)
Lincoln Squarewave 175 TIG(traded it for)
Miller DEL 200 welder/genset
Thermal Dynamics 1250XL plasma cutter
Miller XMT300
I took a bit of time to make the motor plate and mounts, and got a few more of the pipes welded up inside the dash of the car. The dash is pretty crazy looking. My boss (shop owner) did all the pipe layout, he just has me weld them up. :-)
I got pulled off it yesterday to weld up a custom made wishbone for a 4-link setup on a drag truck and machine some bushings for the 4 link brackets. I'll try to post some pictures, if my phone will cooperate...
Vice Grips
WD-40
Duct Tape
Alright, here we go
Ya know, you haven't lived till you've had to use your foot-pedal like a thigh master while kneeling in a car to tack up aluminum tubes...![]()
Vice Grips
WD-40
Duct Tape
Great looking motor plate. Looks a ton better than modifying a generic off the shelf plate.
Everlast Powertig 200DX
Miller Synchrowave 200
Miller Dynasty 300 (Work Machine)
Hobart Handler 210MVP
HTP Microcut 30