Thread: Nervous about my first "real" TIG welding.

  1. #1

    Default Nervous about my first "real" TIG welding.

    Since I don't own a MIG welder, I am going to have to TIG weld my first project.

    I need to build a trailer frame for my teardrop trailer. I am going to use 2" x 2" x 1/8 square tubing.

    Mostly I have practiced with aluminum. Just doing beads. Then I did a few beads on a piece of 1/8 x 1" strip of steel. It did ok, other than when I laid down a bead, the bead was flat, and it was bulged out a little bit on the other side of it.

    I guess that was from too much heat? Or was that ok?

    Just starting out, and doing my first project, just nervous that it won't stay together. LOL.
    Purple Fabricator 211i

  2. #2

    Default

    Also I don't remeber what I had the welder set on. But I was using 1/16 %2 Thor and 1/16 filler. I know I need to go to 3/32 filler. But that was just what I had on hand.
    Last edited by 225; 05-17-2012 at 02:57 PM.
    Purple Fabricator 211i

  3. #3

    Default

    You will for sure want to use 3/32 filler to get a good sized bead going. Post some pics of your welds It hard to tell without seeing the actual weld.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    your tig stick welds to me would be better stick welding a trailer frame stick weld it with 7018
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #5

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    your tig stick welds to me would be better stick welding a trailer frame stick weld it with 7018
    Doesn't 7018's have to be heated in a rod oven or something like that?
    Purple Fabricator 211i

  6. #6

    Default

    no not if its fresh rod lol that just reminded me i need to build a oven for my old welding i mean old over a year old lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #7

    Default

    Right, a fresh sealed pack you should be fine. Got an air tight can to store them in as well. They are around $5 and have a rubber o-ring. Stick will be a little fast and cheaper too.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Default

    whats good for storing welding rod is ammo canisters since there air tight with some moisture packet in the canister
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  9. #9

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    no not if its fresh rod lol that just reminded me i need to build a oven for my old welding i mean old over a year old lol
    Not correct. A new rod doesn't mean it's dry UNLESS it is in a vacuum sealed canister, and then it only considered "dry" for a max of 4 or 8 hours after opening, depending upon the designation of being MR or not. A plastic box with a seal on it, or a cardboard box wrapped in plastic ISN'T considered fresh, unless it has been baked, and then held at the proper temperature until it is used.

  10. #10

    Default

    Link:
    http://www.specialmetalswelding.com/publica/Storage.pdf


    Electrodes which have absorbed excessive moisture should be re-baked in a vented oven at 600ºF ±25°F
    (315ºC±15°C) for one hour or 500ºF±25°F (260ºC±15°C) for two hours. Electrodes must be removed from
    their original containers during this re-baking operation. Electrodes should not be stacked more than 6 layers
    deep on shelves within the oven. Most electrodes can be re-baked at least 2-3 times without substantially
    affecting both the integrity of the flux coating and their welding performance. Following the re-baking operation
    the electrodes should be allowed to cool to room temperature prior to use.
    A common problem that may occur is the uneven absorption of moisture by the electrodes. For example, electrodes
    exposed overnight may exhibit "fingernailing" (uneven burn-off on one side of the electrode) problems
    during welding when used the next day. In this instance the reason that "fingernailing" occurs is due to moisture
    being absorbed by only one side of the electrode causing that side to burn off more slowly and unevenly.
    Correct storage conditions will prevent this type of "fingernailing" problem.
    Purple Fabricator 211i

  11. #11

    Default

    I am going to buy some 7018 1/8 rods, and also some 3/32 filler metal. Then I will cut some small pieces when I get the steel, and do some test runs on both, and see which one comes out better.
    Purple Fabricator 211i

  12. #12

    Default

    Great info.

    Stick welding would definitely be easier and faster, but you could still throw in some TIG welds to get some practice.
    "Engineering is the art of modelling materials we do not wholly understand, into shapes we cannot precisely analyze so as to withstand forces we cannot properly assess, in such a way that the public has no reason to suspect the extent of our ignorance."

    - Dr. AR Dykes

  13. #13

    Default

    Quote Originally Posted by 225 View Post
    I am going to buy some 7018 1/8 rods, and also some 3/32 filler metal. Then I will cut some small pieces when I get the steel, and do some test runs on both, and see which one comes out better.
    7018AC runs like a champ with Everlast Welders. Runs like 7018 but not as prone to moisture.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  14. #14

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    7018AC runs like a champ with Everlast Welders. Runs like 7018 but not as prone to moisture.
    Actually both types of 7018 have moisture problems. It's not so much with how smooth the rod welds, though moisture can cause extra sticking....It's that it will lay down a perfect looking weld on the surface, but in the long run, it will cause under bead hydrogen cracking right at the edge of the penetration. The moisture bound up in the rod is converted to hydrogen, during the welding process and creates something known as hydrogen embrittlement.

  15. #15

    Default

    Click image for larger version. 

Name:	ALOV89ShopOven.jpg 
Views:	537 
Size:	8.4 KB 
ID:	6685not dry rod can be a pain when welding hard facing rod is real bad when damp i have a engine and head oven in my machine shop i keep my rod in it since always have dry rod at 450 and above when i use oven it drys rod good it will go up to 900 degrees
    Last edited by Rodsmachineshop; 05-18-2012 at 01:54 AM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  16. #16

    Default

    I might just wait until I have my I-MIG 205 in hand. There's really no rush on doing the frame. I still have to do a lot to the bottom of the teardrop and then a few other things before I bolt it down to the trailer.

    I am saving up to buy the I-MIG 205 and a Power Plasma 50 at one time.

    Until then, I will keep getting seat time with my 200DX.

    I know it take a lot of seat time to get really good at TIG welding. Since I am just starting out, I am taking my time.
    Purple Fabricator 211i

  17. #17

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    Click image for larger version. 

Name:	ALOV89ShopOven.jpg 
Views:	537 
Size:	8.4 KB 
ID:	6685not dry rod can be a pain when welding hard facing rod is real bad when damp i have a engine and head oven in my machine shop i keep my rod in it since always have dry rod at 450 and above when i use oven it drys rod good it will go up to 900 degrees
    I could just bake a few rods at a time (20 or so) for the welding I am doing. Then one day buy a oven.

    I tried welding some 7018 not out of the oven and it stuck all the time and welded like crap.
    Purple Fabricator 211i

  18. #18

    Default

    same here buying another plasma cutter and spool gun
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  19. #19

    Default

    How do you like the Power Plasma 50?
    Purple Fabricator 211i

  20. #20

    Default

    well put it this way just bought another lol hey 2 plasma cutters is better and also just bought a spool gun for my i mig 205 from oleg . the power plasma igbt 50 is great on cutting
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

Similar Threads

  1. Everlast Super200P died. Performed "diode-ectomy". Now it's welding again!
    By jakeru in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 18
    Last Post: 01-27-2015, 09:24 PM
  2. First "real" TIG welding project coming up.
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 12-27-2012, 07:48 PM
  3. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM
  4. TIG Welding 2024 Aluminum ("unweldable" alloy)
    By jakeru in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 05-11-2011, 08:25 PM
  5. "Test pipe" welding
    By jakeru in forum Other Custom Fabrications
    Replies: 3
    Last Post: 03-23-2011, 03:27 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •