Here's what I got with the machine on 120v. oh and all i had was 1/4 steel. amps at 45. air at 65psi.
the welding was all pedal. with 3/32 lant. pure argon. 5 cup.

220v cut
Click image for larger version. 

Name:	220v.jpg 
Views:	370 
Size:	139.2 KB 
ID:	5939

120v cut
Click image for larger version. 

Name:	120v.jpg 
Views:	337 
Size:	142.2 KB 
ID:	5940

120v w/filler
Click image for larger version. 

Name:	120v rod.jpg 
Views:	342 
Size:	139.4 KB 
ID:	5941

120v fused
Click image for larger version. 

Name:	120v fused.jpg 
Views:	357 
Size:	130.1 KB 
ID:	5942

The machine didn't hiccup at all. hope this helps.