Does Everlast sell/make a drag tip for the S45 torch?
Also, after reading the the Trafimet .pdf, it looks like the PD0116-06 tip is rated at 20 amps and would work better when operating on 120V, has anybody tried this tip on 120V?
Does Everlast sell/make a drag tip for the S45 torch?
Also, after reading the the Trafimet .pdf, it looks like the PD0116-06 tip is rated at 20 amps and would work better when operating on 120V, has anybody tried this tip on 120V?
__________________________
Everlast Power I-MIG 200
Everlast PowerUltra 205P
Everlast SM 200-N
Thermal Dynamics Cutmaster 42
Click for>EVERLAST YOUTUBE CHANNEL VIDEOS
PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.
Thanks zoama585, I have looked at those and may ordr from there. I believe Harbor Freight has the tips and electrodes locally. If I can't get them locally, I may order from China.
I am hoping someone has tried the smaller tip and it works well on 120V.
I am also curious how well it works as a drag tip.
__________________________
Everlast Power I-MIG 200
Everlast PowerUltra 205P
Everlast SM 200-N
Thermal Dynamics Cutmaster 42
We use the SK25 Plasma torches for our 110v PowerPlasma 25 . ( the big difference is in the torch itself not consumables) the torch runs at 25-30 psi and uses about 25% (33lpm) of the flow compared to the S45
with the tips and you will not see a difference in cutting quality, if any thing getting them from the Chinese Supplier ( most come from Wenzhou ) may not be the best idea.
Your best bet is to call the US office and ask them to check with the supplier as i am not up to date on the Sizes they currently make as for some reason it seems lately we have been getting our consumables and such directly from Trafimet .
This post has reminded me i need to ask why all our consumables are Italian and not from our chinese supplier as the quality from them is excellent .
Cheers
Duncan
Here is some more information I have found:
Trafimet S45 Consumable List
These appear to be pilot arc parts:
PR0110 Electrode
PD0116-06 Cutting Tip 20 Amp
PD0116-08 Cutting Tip 30 Amp
PD0116-09 Cutting Tip 40 Amp
These appear to be drag tip parts:
PR0106 Electrode Extended
PD0103-09 Cutting Tip Extended
Last edited by kenwhite; 03-20-2012 at 10:48 AM. Reason: Add drag/pilot comments
__________________________
Everlast Power I-MIG 200
Everlast PowerUltra 205P
Everlast SM 200-N
Thermal Dynamics Cutmaster 42