Thread: Homemade hubs for RWD independent suspension.

  1. #1

    Default Homemade hubs for RWD independent suspension.

    I have been working on these hubs for over a year. They are for a project that I started over 3 years ago right after I graduated high school. I got a Suzuki gs550 engine off of ebay and started building a go-kart frame around. 3 years later, I have learned so much that I realised that using hot rolled square tubing wasn't going to cut it. Currently, its all in limbo. Im trying to decide what I'm going to do with the mess I created over 3 years.

    Hub. The main shaft is made form 8620 alloy steel. I want to have them case hardened so the seal doesn't wear out the shaft. the outer housing is a piece of unknown alloy steel that was about 2.25'' in diameter. I know from welding in a mis-drilled hole in another project that this alloy is hardenable. It cuts kind of like a grade 8 bolt. I made a custom boring bar to cut out the center to size. The bearing are just trailer bearings. The hub fits a standard metric ATV tire. I believe its a 115 mm bolt pattern. The driven side of the shaft has an adapter that goes form the 7/8'' shaft to the 1.25'' universal joints i have.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	downsdfsd.jpg 
Views:	804 
Size:	88.1 KB 
ID:	5384   Click image for larger version. 

Name:	CIMG2949.jpg 
Views:	566 
Size:	49.8 KB 
ID:	5385   Click image for larger version. 

Name:	CIMG2950.jpg 
Views:	557 
Size:	44.2 KB 
ID:	5386   Click image for larger version. 

Name:	CIMG2951.jpg 
Views:	562 
Size:	44.3 KB 
ID:	5387   Click image for larger version. 

Name:	CIMG2952.jpg 
Views:	554 
Size:	42.0 KB 
ID:	5388  

    Click image for larger version. 

Name:	CIMG2953.jpg 
Views:	602 
Size:	41.4 KB 
ID:	5389   Click image for larger version. 

Name:	CIMG2954.jpg 
Views:	518 
Size:	50.2 KB 
ID:	5390   Click image for larger version. 

Name:	CIMG2955.jpg 
Views:	516 
Size:	42.3 KB 
ID:	5391  
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  2. #2

    Default

    Quote Originally Posted by welderdude View Post
    Im trying to decide what I'm going to do with the mess I created over 3 years.
    I wouldn't call it a mess... looks like you've got some time invested there.. good job!
    Everlast PowerPlasma70
    Hobart Ironman 230
    Lincoln A-D/C 225
    'Classic' Everlast Powertig 200DX 'We don't need no steenkin pre-flow..'
    jakemateer.com

  3. #3

    Default

    Hey thanks! I have put tons of time into it. It amazing what I have learned from taking on this kind of project.

    I do know that I will have to re weld a lot of joints that aren't done correctly. When I made most of the cage, I only had a HF 90 amp mig and didn't know enough to use it to its fullest. I will probably invest in the rage 3 compound miter chop saw when I finally decide to start working on it again. Having to cut compound miter cuts with an angle grinder just sucks every bit of fun out of it.

    Right now, I'm thinking about using what I already have and kind of rebuilding it into something even cooler. I just wish I had some real tubing and a tube bender, but that will come later when I have some money to throw around.
    Last edited by welderdude; 02-25-2012 at 04:29 PM.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  4. #4
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Wow, look at that double a-arm front suspension! I'll bet you have learned a lot working on this.

    Have you looked at formula SAE racecars? They have some very cutting-edge designs, for a similar size vehicle and powerplant. They run on paved surfaces, not off-road.

    A rear independent suspension, combined with adding triangulation to the frame, will open the door to tuning the suspension and making it handle more predictably, whether you intend to use this on paved or off-road application.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  5. #5

    Default

    I checked out the formula SAE cars. That is pretty much what I had in mind when I started this project. I liked the idea of being able to run on concrete and then change springs and run on rough dirt. Now that I have thought things over, I think I'm going to try and finish what I have started.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  6. #6

    Default

    your go cart must really fly with that engine in it!!!
    Gil
    powerpro 256
    lincoln 185

  7. #7
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default Nice Project, Dude!!

    I happened across this today and I'm asking myself "why haven't I started my project like this yet? You will have one hell of a fun toy when finished, no matter where you run it. As far as the heat treating for seal wear, ask yourself:"will I put enough miles on this thing to actually wear it out?" The reason I say is that typically in a situation such as this, you got a lot of more important things to worry about than whether a seal is going to wear a groove in 5,000 miles or 50,000 miles. If you see yourself getting 20,000 miles or more out of it, go for it. If not, don't sweat it, unless you just want to do it for a learning exercise. Either way, nice job!! Keep us posted.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  8. #8

    Default

    Thanks hooda! I've decided that unless I acquire the proper heat treating equipment, I'll most likely end up screwing them up. They should be plenty strong the way they are now. If it ever becomes an issue, I'll redesign them and make it better.

    On another note, taking on a project like this has given me new respect for engineers. Its amazing how much thought goes into each little part to make it work like it should.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  9. #9
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Any thoughts for a roll cage? Or is it wide and low enough that it doesn't need one?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  10. #10

    Default

    It has most of one now. Here are some fresh pictures of it. Its finally warm enough for me to start on it again.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	CIMG3003.jpg 
Views:	472 
Size:	51.7 KB 
ID:	5752   Click image for larger version. 

Name:	CIMG3001.jpg 
Views:	503 
Size:	48.6 KB 
ID:	5751   Click image for larger version. 

Name:	CIMG3000.jpg 
Views:	482 
Size:	42.2 KB 
ID:	5750  
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  11. #11
    Join Date
    Feb 2011
    Location
    Fridley, Minnesota
    Posts
    376

    Default

    Hey Dude, Any progress on this lately? The reason I ask is that I've been giving serious thought to starting a project to do a Harley-Powered Can-Am Spyder type setup (reverse trike). Only thing is that I've seen a few of these up close, and they're so well engineered, that I'm almost scared off the idea. I wouldn't want to invest a ton of design time into something that's not completely roadworthy.
    "It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House

    Everlast PowerTig 250EX-arrived 1-26-2012
    Everlast PowerCool W300-arrived 1-26-2012
    Everlast PowerTig 185 Micro-arrived 1-26-2012
    Everlast PowerPlasma 70-arrived 1-26-2012
    ESAB MigMaster 250-borrowed
    HyperTherm 151 AKA "The Light Sabre"
    Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
    Purox OXY/ACETYLENE

  12. #12

    Default

    Honestly, I really haven' done anything yet. Ill post some pictures later of the cluster I got my self into with a 93 jeep wrangler. Than darn jeep has kept me busy.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  13. #13
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by welderdude View Post
    Honestly, I really haven' done anything yet. Ill post some pictures later of the cluster I got my self into with a 93 jeep wrangler. Than darn jeep has kept me busy.
    Really cool pictures. It's a good project you've got there. In my opinion, definitely don't give up on what you've started. Have you figured out how the motor will be mounted?

    Looking forward to what you are getting yourself into. If the cart is any indication, your Jeep working will be pretty interesting to hear about too!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  14. #14

    Default

    The motor is mounted to the frame. I had a solid axle before and was able to drive around my dad's yard. It was pretty quick for how heavy it is. I am really tempted to scrap the current frame and get some real DOM tubing and follow the same design. I really like the flow of the frame. It has a mean stance. I will keep the same Indy/F1 style independent dual suspension.

    Whats amazing is how I realised just how little I knew when I started this project over 3 years ago. I'm waiting until I have a garage I can keep it in. Having to work on it outside just kills my motivation and plus you never know what the weather will do here in illinois. If you dont like it, just wait a few hours, cause it will change
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  15. #15
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by welderdude View Post
    The motor is mounted to the frame. I had a solid axle before and was able to drive around my dad's yard. It was pretty quick for how heavy it is. I am really tempted to scrap the current frame and get some real DOM tubing and follow the same design. I really like the flow of the frame. It has a mean stance. I will keep the same Indy/F1 style independent dual suspension.

    Whats amazing is how I realised just how little I knew when I started this project over 3 years ago. I'm waiting until I have a garage I can keep it in. Having to work on it outside just kills my motivation and plus you never know what the weather will do here in illinois. If you dont like it, just wait a few hours, cause it will change
    Having to work outside is a pain. I'm in the same boat. Unfortunately, in the northwest, the weather isn't terribly accommodating. Pretty wet to be shooting electric arcs.

    You made a good decision designing in the front suspension like you did. Every thought about changing the solid axle in the back? Would be more complicated but might make it worth your while.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  16. #16

    Default

    Looks like it would make a good rat rod gocart!
    http://www.facebook.com/CBRMetalworks

    '96 Tacoma V6 on 37's, full custom, built for racin!
    Yamaha Rhino w/ 800 Rotax built for racin!
    Miller 251 MIG
    Everlast Powerplasma 60C with CNC plasma table

    Looking for sponsors for KOH 2013 race!
    Racin' Tacoma Build Thread

  17. #17
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Another option if you are concerned about seal wear, is to just use hub savers. They are a very thin hard stainless steel sleeve that presses on to the wear area. They are meant to repair hubs with deep seal grooves worn in them. Since you used standard trailer bearings, I'm sure you can find them. They also use the same type of system to repair harmonic balancers on engines with seal grooves worn in them. They are thin enough that you can use the same size seal, it will just have a little more tension on the slightly larger diameter shaft.
    Long arc, short arc, heliarc and in-the-dark!

  18. #18

    Default

    I would leave the square tube frame rails and cut off everything above the frame rails. Build you a round tube cage and let her eat! There's a lot of race car frames built from mild steel; if you build it right it will be safe. I would look into some type of external reverse transmission, like the ones used on heavy trikes or Honda Gold Wing. It will be a pain in the but getting out to push it backwards. It has a cool factor fo-sho!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  19. #19

    Default

    Quote Originally Posted by Tacoma747 View Post
    Looks like it would make a good rat rod gocart!
    I was thinking that as well.. lol

    Thanks for posting pics!
    I've been working on plans for a 2 seater buggy with a GSXR 1000 motor in it. I've got the motor but my big hold up is the hub for independant suspension in the rear. I need a disc brake on one side and a sprocket on the other...

    I'm planning a mid sized sand rail with paddles. We have a riding area close that is all chat from the old lead mines, basically about double the grain size of sand.

    This is not mine, just a sample of what I'm planning....
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  20. #20

    Default

    Oh come on... Got to have something with some power to it... How about my toy??? I didn't make it... Just have had it for years. I have rebuilt it several times. Putting in rear seals right now... I broke the ring gear and snapped the axle... Some awesome wheelies... Straight pipe exhaust baby!!!!
    Click image for larger version. 

Name:	100_6520.jpg 
Views:	929 
Size:	153.8 KB 
ID:	7104
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

Similar Threads

  1. Homemade Tig water cooler
    By welderdude in forum General Welder Questions
    Replies: 35
    Last Post: 02-01-2013, 02:09 PM
  2. Aluminum mountain bike rear suspension TIG weld repair
    By jakeru in forum Welding Repairs
    Replies: 13
    Last Post: 06-21-2012, 01:06 PM
  3. Made collets for my homemade TIG torch...
    By blasphemy000 in forum General Welder Questions
    Replies: 5
    Last Post: 09-30-2011, 01:43 AM
  4. AC DCEN/DCEP independent current control on PP256?
    By acannell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 14
    Last Post: 10-17-2010, 03:43 AM
  5. Water Cooler (homemade)
    By performance in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 07-20-2010, 01:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •