Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 35

Thread: What to use to cut Diamond Plate sheets?

  1. Default What to use to cut Diamond Plate sheets?

    I want to tig some diamond plate boxes out of 4 x 8 sheets of aluminum diamond plates. What do you recommend to use to rip and cut the sheets?

  2. #2

    Default

    If you have a local place like I have, and did get them to do today, that can do it for little or nothing, and include the cost of the sheets: A laser CNC cutter...Otherwise, if it's thin enough a table saw with a fine blade.

  3. Default

    Quote Originally Posted by performance View Post
    If you have a local place like I have, and did get them to do today, that can do it for little or nothing, and include the cost of the sheets: A laser CNC cutter...Otherwise, if it's thin enough a table saw with a fine blade.
    yes, it is thin .063 aluminum. Can you use a table saw with a non ferrous blade? I heard that it may kick up a lot?

  4. #4

    Default

    Isn't this what Everlast says their plasma cutter is so good at on their You Tube video?

    Basically, you need a plasma cutter. Specifically, an Everlast Plasma Cutter.

    Now, where's my commission?

  5. #5

  6. Default

    Ive never heard of using a table saw. But I know that you can use a circular saw in a pinch if thin enough too. Never tryed it though. If ya do Id use some strait edge as a guide.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  7. Default

    Quote Originally Posted by jp2code View Post
    Isn't this what Everlast says their plasma cutter is so good at on their You Tube video?

    Basically, you need a plasma cutter. Specifically, an Everlast Plasma Cutter.

    Now, where's my commission?
    I actually have a Everlast Plasma, however, I am looking for exact square and precise cuts. Thanks anyway...

  8. #8

    Default

    Use a blade made for aluminum and go slow. Or you could try a pneumatic shear. If you live near a fab or welding shop you could see if they are willing to do it cheap. If you brought it to my shop I would do it for a beer.
    Power tig 225lx
    Hand tools up the wazoo.

  9. #9

    Default

    You can make square precise cuts with the plasma cutter. I use a straight edge clamped onto the metal as a guide.
    I drag the torch top along the side. Take your time and the cuts will be precise as anything else.
    Power tig 225lx
    Hand tools up the wazoo.

  10. Default

    Quote Originally Posted by dyethor View Post
    Use a blade made for aluminum and go slow. Or you could try a pneumatic shear. If you live near a fab or welding shop you could see if they are willing to do it cheap. If you brought it to my shop I would do it for a beer.
    Thanks. I have used a skill saw with a non ferrous blade and it does ok with a straight edge. Just looking for a more precise cut. Thanks for all of the feedback. How do the pneumatic shears work?

  11. Default

    Quote Originally Posted by dyethor View Post
    You can make square precise cuts with the plasma cutter. I use a straight edge clamped onto the metal as a guide.
    I drag the torch top along the side. Take your time and the cuts will be precise as anything else.
    Do you use a guard on the plasma cutter?

  12. #12

    Default

    I have a different brand plasma cutter it has a brass tip. I drag the side of the tip along the straight edge. The shears cut using a scissor action. not good for making any sharp radius's only large ones and straight cuts.
    Power tig 225lx
    Hand tools up the wazoo.

  13. #13
    Join Date
    Feb 2012
    Location
    San Diego county
    Posts
    10

    Default

    I've cut aluminum sheet with regular wood working tools. I don't use my best blades, but it works fine. That goes for tablesaw, compound miter saw, etc. I'd wear a face shield and maybe long sleeves. You can get pelted with chips.

    Doug

  14. Default

    Quote Originally Posted by DWSD View Post
    I've cut aluminum sheet with regular wood working tools. I don't use my best blades, but it works fine. That goes for tablesaw, compound miter saw, etc. I'd wear a face shield and maybe long sleeves. You can get pelted with chips.

    Doug
    Thanks Doug!

  15. #15
    Join Date
    Feb 2012
    Location
    San Diego county
    Posts
    10

    Default

    Quote Originally Posted by Buggy Chief View Post
    Thanks Doug!
    you bet. good luck! How much is a sheet for 4'x8' diamond plate?

    Doug

  16. Default

    Quote Originally Posted by DWSD View Post
    you bet. good luck! How much is a sheet for 4'x8' diamond plate?

    Doug
    Just paid $200/ sheet and then found for $92/sheet. All still seems expensive. How much in your neck of the woods?

  17. #17

    Default

    The diablo non-ferrous blade is a beast at cutting aluminum. I have cut 1/4" tubing with no problem.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  18. Default

    Has anyone cut steel with a circular saw?
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  19. #19

    Default

    I haven't used it but they make a diablo blade called a steel demon and it says don't use on thicker than 1/4". Even a 1/4" though is not bad for a saw.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  20. Default

    Hmm it just seems it would be a kinda handy way to cut stuff here and there. I wouldnt use it on my good saw though. What about putting a metal blade on a wood band saw. Would that be any good to use or does the wood bandsaws not have a big enough motor on them.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •