Thread: Sean Murphy Project 1 - Header repair for a dirt late model

  1. #1

    Default Sean Murphy Project 1 - Header repair for a dirt late model

    My best friend runs a Nesmith Dirt Late Model. This is a GM crate motor series. He wanted to race really bad and borrowed an old set of headers. They were cracked pretty good and very rusty. This was a I just want to race tonight fix. These headers had been raced for 3 years by another friend, and needless to say we picked them out of the scrap pile. I did a little grinding, but not a major cleanup these headers were thin!

    Power Arc 140st
    27-32 amps

    This is the first hole that I plugged

    This was my first tig welds with my Power Arc 140st




    Everlast Power Arc 200 --> Money Maker$$
    Everlast Power Arc 140ST
    Everlast IMig 200
    Everlast Power Tig 225lx
    Everlast Power Super Cut 50
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Everlast PowerTig 200DX - Sold! Fantastic Machine!
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press
    Powerhouse 7000 watt generator


    www.murphywelding.com

  2. #2

    Default

    did you backpurge the pipes?
    Some of the crap I use to keep busy:

    Everlast 200DX
    Millermatic 211 Mig
    Hypertherm Powermax 30 plasma cutter
    Lincoln Weld-Pak 100
    Century Stick welder
    Oxy set-up with Henrob 2000 torch
    Logan 200 lathe (60 years old)
    Jet band saw
    About 6 Harbor Freight grinders with different discs/wheels/brushes

  3. #3

    Default

    Real tough to weld old headers after they been heated and cooled a thousand times get real thin. What size wire did you use and what gas flow did you use? Good job for what you had to work with.
    Bill

  4. #4

    Default

    no, these were junky! this was a get me through the night so I can race.
    Everlast Power Arc 200 --> Money Maker$$
    Everlast Power Arc 140ST
    Everlast IMig 200
    Everlast Power Tig 225lx
    Everlast Power Super Cut 50
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Everlast PowerTig 200DX - Sold! Fantastic Machine!
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press
    Powerhouse 7000 watt generator


    www.murphywelding.com

  5. #5

    Default

    Quote Originally Posted by 67cudafb View Post
    Real tough to weld old headers after they been heated and cooled a thousand times get real thin. What size wire did you use and what gas flow did you use? Good job for what you had to work with.
    1/16 tig rod, and I believe 1/16 or 3/32 2% tungsten
    Everlast Power Arc 200 --> Money Maker$$
    Everlast Power Arc 140ST
    Everlast IMig 200
    Everlast Power Tig 225lx
    Everlast Power Super Cut 50
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Everlast PowerTig 200DX - Sold! Fantastic Machine!
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press
    Powerhouse 7000 watt generator


    www.murphywelding.com

  6. Default

    Not bad at all.
    I am in the middle of building a set of headers for my S10.
    I'm putting a 598 BigBlock in it.
    I've built 2 others BigBlock S10's but, I'm not going to pay 1200.00 for a set of headers again.
    Miller 135 Mig
    Miller 211 Mig (Broken)
    Lincoln SP-180T MIG (Wont hold gas)
    HTP MicroCut 875S Plasma Cutter
    HTP Invertig 201 TIG Welder
    JET 7"x12" Horizontal/Vertical Bandsaw
    G0704 Mill "BF20" (Working on CNC Conversion)
    Hypertherm Powermax 1000G3 w/ Machine Torch, 6'x10' CNC Water Table
    Custom Built 5'x5' CNC Router Table w/ Milwaukee 3-1/2 HP Production Router
    South Bend 9" Bench Top Lathe Model C
    South Bend 14"x40" Engine Lathe
    South Bend 9"x32" Vertical Mill
    JD2 Model 32 Bender with Dies

  7. #7

    Default

    I saw this online don't know if it will help http://www.summitracing.com/expertad...ustom-Headers/ Also have seen plastic mock up like round legos in Hot Rod magazine but can't find the maker of these I will look for it and post it when I find it and I thought $699 was bad for a set of TTI headers.
    Bill

  8. #8

    Default

    Quote Originally Posted by Joe from NY View Post
    did you backpurge the pipes?
    you dont need to backpurge when welding steel
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  9. #9

    Default

    man, i would have wasted all that gas..
    Some of the crap I use to keep busy:

    Everlast 200DX
    Millermatic 211 Mig
    Hypertherm Powermax 30 plasma cutter
    Lincoln Weld-Pak 100
    Century Stick welder
    Oxy set-up with Henrob 2000 torch
    Logan 200 lathe (60 years old)
    Jet band saw
    About 6 Harbor Freight grinders with different discs/wheels/brushes

  10. #10

    Default

    Quote Originally Posted by Diabolical View Post
    Not bad at all.
    I am in the middle of building a set of headers for my S10.
    I'm putting a 598 BigBlock in it.
    I've built 2 others BigBlock S10's but, I'm not going to pay 1200.00 for a set of headers again.
    If I were going to build a set I would copy a tri-y design. There's a guy in Alabama who has a company Rapture Carburetor, and he came up with the design/idea. He was some type of industrial carburetor specialist who fell into the racing deal on accident. Started building headers and put them on while engines where on the dyno. Literally kept trying different things until he got the numbers he wanted. A friend purchased a set of his headers and a carb; it literally woke the engine up!
    Everlast Power Arc 200 --> Money Maker$$
    Everlast Power Arc 140ST
    Everlast IMig 200
    Everlast Power Tig 225lx
    Everlast Power Super Cut 50
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Everlast PowerTig 200DX - Sold! Fantastic Machine!
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press
    Powerhouse 7000 watt generator


    www.murphywelding.com

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •