Thread: welding cast to stainless

  1. #1

    Default welding cast to stainless

    I'd like to weld stainless(304) v-band flanges on the exhaust manifolds of the 2-stroke saabs I work on for better sealing and easier disconnect. I've only welded mild to cast iron or cast iron to itself, any thoughts? because 'cast' rod is mostly nickel anyway (55 or 99%) I can't see much of a problem using a high-nickel stick rod, but I figure I'll solicit opinions anyway.

    this is also probably thick enough that I can TIG it with the I-MIG, though, so if anyone has a dynamite TIG filler for welding 304 stainless to highly carbon-impregnated cast iron, I'm all for it
    McGuire Irvine
    Crow Motor Co.

    Lincoln powermig 225 (work)

  2. #2

    Default

    Wouldn't it be easy to just make a stainless exhaust manifold for it ?

    PP 256 (SOLD) : 2013 250EX : I-MIG 250P/w 20' Profax gun : Power Plasma 60/w p80 torch : Hobart Handler 135/w 12' .023" Profax gun : 3M Speedglas 9100XX
    I'm not an expert or an Everlast employee, I'm just a hobby welder sharing my experience and helping where I can.

  3. #3

    Default

    yes and no. we have upwards of 40 cast manifolds(stainless is expensive, boss is cheap) and re-designing 2-stroke exhaust ahead of the expansion chamber is a big headache that I'm not ready to tackle yet, so factoring those things in it's much easier to weld a new modern flange on the mani and the downpipe. when I do get around to redoing the manifold in stainless, I'll probably move the joint down outside the belly pan closer to the expansion chamber so the exhaust is easier to handle.

    worse case I can use mild steel flanges, I was going to use stainless to the sealing surface wouldn't corrode and start leaking.
    McGuire Irvine
    Crow Motor Co.

    Lincoln powermig 225 (work)

  4. #4

    Default

    Expansion differential is so different, I'd imagine something would crack even if the weld was solid.

  5. #5
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    761

    Default

    Although I have never attempted welding stainless to cast, my gut tells me: stick or TIG weld with nickel rod (and I only have experience with "Nickel 55", which seems suitable) for this.

    The reason nickel rod is good for welding cast iron when cold, is that it doesn't contract from heat as much as other alloys, so it limits the contraction stresses that are applied to the brittle cast parent metal from the cooling weld bead.

    I don't know how much I like the idea of austenitic stainless welded to cast iron, however, due to the differences in thermal expansion of the two materials, combined with the brittleness of cast iron - as already mentioned by Mark. (Even if you got it welded without cracking, it might crack subsequently upon usage - normal heat cycling of an exhaust manifold.

    Mild steel to cast iron would have less potential problems with cracking in this manner (because the thermal expansion coefficients of the materials are a lot closer.)
    '07 Everlast Super200P

  6. #6

    Default

    You might have a better chance if you build up a ledge out of nickel, say 1/4 to 3/8 and then welded the stainless to the nickel ledge, a thought for you to think about.

  7. #7

    Default

    I'm glad I asked, I hadn't thought about the difference in thermal expansion. I'm pretty sure these manifolds are plain grey iron, so figure 5.7 ppm/F. 304&308 are 9.3, 309 is 8.2*
    410, on the other hand, is 6.1. too bad no one makes V-band flanges in 410.

    mild I'm seeing listed at 7.3, and I'm seeing 5.5 for 410 on another reference.

    http://cp.literature.agilent.com/lit...5517-90143.pdf
    http://www.engineeringtoolbox.com/li...ents-d_95.html

    I guess I'll use mild flanges. my other option is to fab a new downpipe and move the v-band under the bellypan.


    *this explains why 309 does well welding 304/308 to mild.
    McGuire Irvine
    Crow Motor Co.

    Lincoln powermig 225 (work)

  8. #8

    Default

    Quote Originally Posted by geezer View Post
    You might have a better chance if you build up a ledge out of nickel, say 1/4 to 3/8 and then welded the stainless to the nickel ledge, a thought for you to think about.
    you're probably right on that one. nickel is ductile enough to disperse enough of the stresses from the stainless' higher coefficient of expansion before they reach the brittle cast iron to keep it from cracking.

    3/8" deposit is probably what, 5-6 passes with 1/8" ni55? should be able to get that out of a lb. I'd like to not have to buy more than a lb for experimentation. that stuff ain't cheap.
    McGuire Irvine
    Crow Motor Co.

    Lincoln powermig 225 (work)

  9. #9
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    761

    Default

    That's interesting that the 4xx series stainless steel is closer to grey cast iron in terms of thermal expansion rate than mild steel is.
    '07 Everlast Super200P

  10. #10

    Default

    I thought so too. I think that might explain it's prevalence in exhaust, too. although, I don't think I've ever seen headers out of 410, where the benefit would be greatest.
    McGuire Irvine
    Crow Motor Co.

    Lincoln powermig 225 (work)

  11. #11

    Default

    400 series stainless doesn't have nickle in it only chromium. That is why it is not a corrosion resistant as 300 series.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  12. #12

    Default

    Quote Originally Posted by Cippee View Post
    400 series stainless doesn't have nickle in it only chromium. That is why it is not a corrosion resistant as 300 series.
    400 series do contain nickle, just not in the high amounts as 300 series.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  13. #13

    Default

    Sorry no it doesn't look. "There are several "types" of stainless steel. The 300 series (which contains nickel) is NOT magnetic. The 400 series (which just contains chromium and no nickel) ARE magnetic."

    Look it up.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  14. #14

    Default

    Hears a link to a chart of different stainless alloy compositions.

    http://www.scotforge.com/charts/sf_s...ainless_ns.htm
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  15. #15

    Default

    Quote Originally Posted by Cippee View Post
    Sorry no it doesn't look. "There are several "types" of stainless steel. The 300 series (which contains nickel) is NOT magnetic. The 400 series (which just contains chromium and no nickel) ARE magnetic."

    Look it up.
    maybe i should have been more specific... ferritic ss dont have nickle. martensetic ones do. 403 408 414 431 to name a few.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  16. #16

    Default

    If you weld cast iron in small runs and let it cool in between runs you can weld it without preheat. Some pieces are too big for me to preheat evenly. Also I tend to be on the lazy side at times. Sorry jerky I didn't mean to sound rude or snotty about the 400 series. I didn't realize how my post sounded until I read it.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  17. #17

    Default

    Quote Originally Posted by Cippee View Post
    If you weld cast iron in small runs and let it cool in between runs you can weld it without preheat. Some pieces are too big for me to preheat evenly. Also I tend to be on the lazy side at times. Sorry jerky I didn't mean to sound rude or snotty about the 400 series. I didn't realize how my post sounded until I read it.
    its ok, i was just trying to get across that some 400's do have nickle, but most dont. as for cast, you also need to "peen" the weld, witch is hitting it with a hammer to allow the deposited weldment to "stretch" so it wont crack when cooling.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  18. #18

    Default

    I did leave out the most important part, thanks. All the fumes I have inhaled are starting to affect my brain. Someone would have been cursing when the weld cracked. Thanks guys.
    Everlast PowerTig 250EX
    Everlast PowerCool 300
    Lincoln Powermig 215
    Magnum SG Spool Gun
    Don't jump on my Gomba

  19. #19
    Join Date
    Mar 2011
    Location
    mission viejo CA
    Posts
    92

    Default

    Quote Originally Posted by Cippee View Post
    I did leave out the most important part, thanks. All the fumes I have inhaled are starting to affect my brain. Someone would have been cursing when the weld cracked. Thanks guys.
    sounds like a 309 filler is in order considering that what it is used for
    Lincoln precision tig 275
    Miller Syncrowave 350 Tig
    Miller 250 Mig
    old miller 200 Mig
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list

  20. #20
    Join Date
    Mar 2012
    Location
    Remote S. Idaho
    Posts
    54

    Default

    You can 'butter' the cast with a real stretchy nickel rod, then weld 312 or 308L to it, but compatibility problems could be very high and carbon monoxide danger very real in case of a crack. Best not.
    There is no safe direction to point an unsafe gun.
    PowerPro 205
    Hobart 250HF
    Powcon 300ST
    gas stuff
    14x60 Hercules Ajax lathe
    Gorton I-22 MastrMil
    Landis 6x18 surface grinder
    20" Powermatic bandsaw
    Ancient, big drill press
    350 pound anvil and a bunch of hammers
    If I can't fix it I can make it.....unrecognizable.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •