    A customer was working on some sort of Honda engine swap, and brought in this intake manifold, asking me to TIG weld closed these small, about 1/8" diameter holes in the cylinder head mounting surface. The customer claimed the holes were related to the original cold starting/running design he wished to eliminate. The holes connected to machined openings for fuel injectors, appearing to supply (or drain) the fuel pressure to those injectors.

    The customer had previously attempted plugging the holes with JB weld (metal powdered expoxy), but the JB weld had failed. I prepped the holes by fileing their ID's clean with a small jewelers file, (shining a flashlight from behind to inspect), and proceeded to TIG weld the holes closed near the mounting surface. As shown in the last picture, I fed a filler rod through from the back side of the hole, to attempt to provide a less protruding weld bead (as the customer had expressed interest in not having to resurface the manifold mounting surface afterwards.) It work *just about* perfectly. As can be expected, the filler rod got stuck from the cooling weld bead, and sheared off neatly by twisting it, and in the front face there was left a recessed "dimple" where the hole had been.

    Customer was happy.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG_0038_small.JPG 
Views:	507 
Size:	58.1 KB 
ID:	1032   Click image for larger version. 

Name:	IMG_0039_small.JPG 
Views:	469 
Size:	53.0 KB 
ID:	1031   Click image for larger version. 

Name:	IMG_0040_small.JPG 
Views:	493 
Size:	51.5 KB 
ID:	1030   Click image for larger version. 

Name:	IMG_0041_small.JPG 
Views:	506 
Size:	53.1 KB 
ID:	1029  
    Last edited by jakeru; 03-06-2011 at 10:55 PM.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  2. #2

    Default

    nice work!
    i have some cool projects like this planned for when my unit arrives!
    300whp FWD 94 Celica
    PowerPro 205 with a hack behind the mask!

Similar Threads

  1. Custom mod 6 liter diesel intake manifold
    By Wrdsk in forum Other Custom Fabrications
    Replies: 0
    Last Post: 10-29-2014, 01:14 AM
  2. Project 1 from Zedron - Honda B16 Intake Manifold
    By zedron in forum On Road Fabrication
    Replies: 12
    Last Post: 03-02-2013, 05:37 PM
  3. Honda CBR 600 F4
    By donor76 in forum On Road Fabrication
    Replies: 3
    Last Post: 09-15-2012, 02:16 PM
  4. Custom Toyota 4-cylinder Intake Manifold (jakeru's #17)
    By jakeru in forum On Road Fabrication
    Replies: 9
    Last Post: 07-31-2011, 12:50 PM
  5. Clogged Intake Manifold Cleaning (jakeru's project #2)
    By jakeru in forum Welding Repairs
    Replies: 9
    Last Post: 06-08-2011, 04:39 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •