mobilewelder
the st140 great welder
by , 01-21-2012 at 01:17 AM (412 Views)
ok so i have put the st140 to the test and would like to say its a great welder i have ran almost 50lb of welding rod though it and i must say it is a great welder have not posted a video but have been welding in a boiler bottom with it and it has worked great i have a 50ft Extension Cord with alligator clips to clip on to power ok in the Manuel for the st140 it says you can not burn 6010 rod and that 6011 is the only one you can burn with it at 120 in put 6011 or 7018 h4r works great the st140 can and will burn 1/8 6010 rod you need 240 volt at the min 30 amp breaker i ran 1/8 6010 at 80 amp welding 5/8 plate works great at full power it burned though 5/8 plate with out beveling i had to turn down the welder al in all a great welder realy happy with it would love to try out some of the other welders on here