Sharing this as a tip I guess, like to see what others do. If this thread is locked PM me.

I had two 4.5" pipes today that needed to be cut at 45 degrees. I can get it close with my eyeball and square. inclinometer and stand-off (or inclinometer and water tank). Then I thought I would look for templates since the internet seems to have it all. I found some really cool magnetic ones, but $100 for them.

http://www.wrapitcut.com/home/

After a lot of searching I found the solution below, on harderwoods.com no less???

http://www.harderwoods.com/pipetemplate.php?f=dn&units=in&paper=letter&theta=45&rmd=600&rbd=4.5&rbt=.1&offset=0&Submit=Submit

I fudged up the number and got what I wanted. Printed, cut and taped up the template. Grease pencil twice. Done.

I also found this below, prior, worth a mentioned as well. But the above one did the trick.