PowerPlasma Series |
|
Inverter Type |
|
Voltage/Phase |
|
Start Type |
|
Pilot Arc |
|
Gouge* |
|
Recommended maximum cut @ 10-12 ipm in steel.** Decrease by 25-30% for Aluminum |
|
Maximum severance cut @ 3 ipm in steel |
|
Typical Use |
|
|
SuperCut 40 |
|
Toshiba/Fuji Mosfet |
|
120/240 V 1phase |
|
High Frequency |
|
NO |
|
NO |
|
3/8" |
|
5/8" |
|
Hobbyist |
|
|
SuperCut 50 |
|
Toshiba/Fuji Mosfet |
|
120/240 V 1phase |
|
High Frequency |
|
NO |
|
NO |
|
5/8" |
|
3/4" |
|
Hobbyist, Artist, Automotive |
|
|
|
PowerPlasma 50 |
|
Infineon IGBT |
|
240 V 1 phase (120/240 optional) |
|
Blowback type Non-HF |
|
YES |
|
NO |
|
3/4" |
|
1" |
|
Automotive, General Repair, Light Industrial, Fabrication, HVAC |
|
|
PowerPlasma 60 |
|
Infineon IGBT |
|
240V 1 phase |
|
High Frequency |
|
YES |
|
Light |
|
7/8" |
|
1 1/8" |
|
Automotive, General Repair, Industrial and Commercial, Fabrication Shop, HVAC, Agricultural |
|
|
|
PowerPlasma 60E |
|
Infineon IGBT |
|
220/240 V 3 phase |
|
High Frequency |
|
YES |
|
YES |
|
1" |
|
1 1/4" |
|
Automotive, Fabrication Shop, Industrial and Commercial, Agricultural |
|
|
PowerPlasma 70 |
|
Infineon IGBT |
|
240V 1 phase |
|
High Frequency |
|
YES |
|
YES |
|
1 1/8" |
|
1 3/8" |
|
General Repair, Industrial and Commercial, Fabrication /Machine Shop, Agricultrual |
|
|
|
PowerPlasma 80 |
|
Infineon IGBT |
|
240V 1 phase |
|
High Frequency |
|
YES |
|
YES |
|
1 1/4" |
|
1 1/2" |
|
General Repair, Industrial and Commercial, Fabrication/Machine Shop, Agricultural |
|
|
PowerPlasma 100 |
|
Infineon IGBT |
|
220/240 V 3 phase |
|
High Frequency |
|
YES |
|
YES |
|
1 5/8" |
|
1 7/8" |
|
Industrial and Commercial |
|
|
|
|
* For Gouging, consult Everlast for special gouging torch and accessories.
* * Piercing capacity is typically 40-50% of recommended cut capacity. |
|
|
Copyright 2004 - 2010 EverlastInc. All Rights Reserved.
While welding is a valuable skill to possess, it is important to get the right machine to do the job. If you are a professional or a hobbyist and are trying to find the machine to fit your needs, Everlast can help. We offer a full line of welders for the hobbyist and professionals, including MIG, TIG, STICK and plasma cutters. We are proud to feature IGBT components and modules from Siemens for long life service whether in the field, in the shop or in the home. Don't forget about our line of silent diesel generators and engine drive welders. We offer convenient ordering capability without leaving your home or office.
|