contact us: 1-877-755-weld(9353) DEALERS WANTED | Terms & Policy
Welder
Welder Home
Search our site
Welder
Welding equipments Everlast Forum Home Contact everlast Everlast FAQ
Welcome to everlast power equipment. Your one stop source for reliable welding and plasma cutting equipments http://www.everlastwelders.ca http://www.everlastwelds.com.au http://www.everlastwelds.eu
Bookmark and Share

PowerTig 225 LX:

 
PowerTig Series CC Inverter: 225 Amp AC/DC Pulse Tig/ 175 Amp DC Stick Welder
Processes: GTAW-P, SMAW
IMPORTANT PRODUCT NOTE: Amps are adjusted on panel with amp control knob for operation with 2T/4T torch switch and foot pedal. To achieve maximum operation capabilities, Everlast includes a water-cooled TIG torch for use with this welder. Most air-cooled torches are limited to 200 amps. Using the water-cooled torch "dry" will damage the torch. A Water Cooler is necessary for use with the stock torch.
 
PowerTig 225 LX

PowerTig 225 LX




      
Features & Benefits
- Stable, smooth arc characteristics with good puddle wet in.
- Portable and lightweight with industrial capability.
- Adjustable weld parameters for 2t/4t operation.
- Pulse function increases weld quality while reducing overall heat input for thin or heat sensitive metals.
- Easy to connect torch and accessories allow quick setup and adjustments.
- Digital readout for accurate setting of Amperage.
- Color coded controls are easy to find and understand.
- Economy 12 ft 18 series water-colled torch torch and accessories.
Special built-in 240V receptacle for use with the optional Everlast PowerCool 300.

NOTE: For geneator use, the generator must produce a MINIMUM 8500 watts of continuous output and be designated as "clean power" by the generator manufacturer. A larger generator may be necessary for best results. Use with a generator not designated as "clean power" by the generator manufacturer may void welder warranty.

Not recommended for stick operation with E6010.
















Make an offer for PowerTig 225 LX  


Price : $1349.00

Recommended Areas Of Use
- Onsite Welding Repair
- Motorsports/ Automotive
- Construction/HVAC
- Commercial/Industrial Maintenance
- Fabrication/Machine Shops
- Shipyard/Pipeline
- Home/Hobby/DIY
- Farm/Ranch/Agricultural
- Gun Smith












Standard Equipment
- 12 ft Economy WP 18 series water-cooled TIG torch
- Work clamp with cable
- SMAW electrode holder(Stub type, subject to change)
- Argon regulator
- Consumable starter pack (Tungsten not included.)
- Foot Pedal
6ft. Input Power Cable (Recommended NEMA 6-50 to be supplied by the customer.)
Optional Equipment
- Water cooler
- Welding cart
- Welding helmet
- Consumable kit
- WP, 9,17, 18, 20 or 26 Series compatible TIG torch, 15ft or 25ft lengths. (Not available for substitution. Additional purchase only.)
-US made foot pedal. (Not available as substitution. Additional purchase only.)
-NEW! 17 SERIES FINGER AMP CONTROLLED TORCH. 15FT. CHECK AVAILABILITY.
Recommended Metals
- Steel
- Aluminum (PowerTig Series only)
- Stainless Steel
- Titanium
- Copper/nickel alloys
- Virtually all weldable metals.
PowerTig 225 LX
PowerTig 225 LX
PowerTig 225 LX
PowerTig 225 LX
PowerTig 225 LX
PowerTig 225 LX
PowerTig 225 LX
PowerTig 225 LX
Power I-Tig 200
PowerTig 185 Micro
PowerTig  200DX
PowerTig 225 LX
PowerTig  250EX
PowerTig 315LX
Power I-Tig 200 PowerTig 185 Micro PowerTig 200DX PowerTig 225 LX PowerTig 250EX PowerTig 315LX
OUTPUT POWER TYPE DC DC/AC DC/AC DC/AC DC/AC DC/AC
MINIMUM AMP START ON DC/AC 5 A (UNIT IS DC ONLY) 5 A/20 A 5 A/20 A 5 A/20 A 5 A/5 A 10/ 20 A
TIG(GTAW) AMPS/VOLTS @ DUTY CYCLE 200 A, 18 V @ 35%
160 A, 16.4 V @ 60%
130 A, 15.2 V @ 100%
185 A, 17.4 V @ 35%
125 A, 15 V@ 60%
100 A, 14 V @ 100%
200 A, 18 V@ 60%
160 A, 16.4 V @ 100%
-
225 A, 19 V @ 60%
175 A, 17 V @ 100%
-
250 A, 20 V @ 60%
200 A, 18 V @ 100%
-
315 A, 22.6 V @ 60%
250 A, 20 V @ 100%
-
TIG OPEN CIRCUIT VOLTAGE (OCV) 70 V 70 V 70 V 70 V 70 V 70 V
STICK (SMAW) AMPS/VOLTS @ DUTY CYCLE 160 A, 26.4 V @ 35%
130 A, 25.2 V @ 60%
100 A, 24 V @ 100%
NO STICK CAPABILITY 160 A, 26.4 V @ 35%
130 A, 25.2 V @ 60%
100 A, 24 V @ 100%
175 A, 27 V @ 35%
135 A, 25.4 V @ 60%
105 A, 24.2 V @ 100%
200 A, 28 V @ 35%
160 A, 26.4 V @ 60 %
130 A, 25.2 V @ 100%
250 A, 30 V @ 35%
200 A, 28 V @ 60%
160 A, 26.4 V
STICK OPEN CIRCUIT VOLTAGE (OCV) 70 V N/A 70 V 70 V 70 V 70 V
INPUT VOLTAGE/PHASE/Hz 110-120/220-240 V 1 PH 50/60 Hz 220-240 V 1 PH 50/60 Hz 220-240 V 1 PH 50/60 Hz 220-240 V 1 PH 50/60 Hz 220-240 V 1/3 PH 50/60 Hz 220-240 3 PH 50/60 Hz
INPUT AMPS MAX INRUSH (I1MAX )@ AVAILABLE VOLTAGE 30 A @ 220 V
28.7 A @ 230 V
27.5 A @ 240 V
24.5 A @ 220 V
23.1 A @ 230 V
22.1 A @ 240 V
33.6 A @ 220 V
32.1 A @ 230 V
30.8 A @ 240 V
39 A @ 220 V
37 A @ 230 V
35 A @ 240 V
45 A/26 A @ 220 V 1/3 PH
43 A/24 A @ 230 V 1/3 PH
40 A/22 A @ 240 V 1/3 PH
32.8 A @ 220 V
31.4 A @ 230 V
30 A @ 240 V
INPUT AMPS MAX RUNNING AMPS (I1EFF ) 24 A @ 220 V
23 A @ 230 V
24 A @ 240 V
14.5 A @ 220 V
13.6 A @ 230 V
13 A @ 240 V
27 A @ 220 V
26 A @ 230 V
25 A @ 240 V
31 A @ 220 V
30 A @ 230 V
29 A @ 240 V
36 A/16 A @ 220 V 1/3 PH
34 A/15 A @ 230 V 1/3 PH
32 A/15 A @ 230 V 1/3 PH
25.4 A @ 220 V
24.3 A @ 230 V
23.2 A @ 240 V
APPROX. UNIT WEIGHT (POUNDS) 32 40 59 62 65 105
DIMENSIONS (WxLxH) 7.25"x16.25"x12.75" 7.25"x19"x12.75" 9"x21"x17" 9"X21"x17" 9"x21"x17" -
FEATURES
FOOT PEDAL YES/ OVERIDES PANEL AMPS WITH FULL RANGE OF AMPS AVAILABLE AT PEDAL. NO LIMIT (SUBJECT TO CHANGE. CONSULT EVERLAST.) YES/OVERIDES PANEL AMPS WITH FULL RANGE OF AMPS AVAILABLE AT PEDAL. NO LIMIT (SUBJECT TO CHANGE. CONSULT EVERLAST) YES/OVERIDES PANEL AMPS. SET/LIMIT MAX AVAILABLE AMPS ON WITH KNOB ON PEDAL. YES/ SET MAX AVAILABLE AMPS WITH PANEL AMP KNOB. YES/ SET MAX AVAILABLE AMPS WITH PANEL AMP KNOB. YES/ OVERIDES PANEL AMPS SET/LIMIT MAX AVAILABLE AMPS WITH KNOB ON PEDAL.
STICK ARC FORCE CONTROL YES N/A NO NO YES YES
LIFT START TIG YES NO YES YES YES YES
HF START TIG YES YES YES YES YES YES
SPOT TIMER NO NO NO NO 0-10 SECONDS NO
2T/4T TORCH TRIGGER PANEL CONTROL YES 2T OR PEDAL ONLY YES YES YES YES
START AMPS (2T/4T TRIGGER FUNCTION) NO, FIXED NO NO, FIXED NO, FIXED 5-100 A NO, FIXED
END AMPS (2T/4T TRIGGER FUNCTION) NO, FIXED NO NO, FIXED NO, FIXED 5-100 A NO, FIXED
UP SLOPE (2T/4T TRIGGER FUNCTION) 0-5 SECONDS NO NO 0-10 SECONDS 0-10 SECONDS 0-15 SECONDS
DOWN SLOPE (2T/4T TRIGGER FUNCTION) 0-5 SECONDS NO 0-5 SECONDS 0-10 SECONDS 0-10 SECONDS 0-30 SECONDS
PRE FLOW (GAS) 0-5 SECONDS AUTO .3 SECONDS FIXED .3 SECONDS 0-10 SECONDS 0-10 SECONDS 0-10 SECONDS
POST FLOW(GAS) 0-25 SECONDS AUTO 2-3 SECONDS 0-25 SECONDS 0-25 SECONDS 0-25 SECONDS 0-10 SECONDS
TIG AC FUNCTIONS
AC FREQUENCY CONTROL NO AC CAPABILITY 20-250 Hz 20-250 Hz 20-250 Hz 20-250 Hz 20- 500 Hz
AC BALANCE CONTROL NO AC CAPABILITY 10-90% 30-70% 30-70% 10-90% 10-90%
TIG PULSE FUNCTIONS
PULSE FREQUENCY RANGE .2-250 Hz NO PULSE FUNCTION .2-25 Hz .2-25 Hz . 2-500 Hz .2-750 Hz
PULSE AMP CONTROL RATIO CONTROLLED: 5-95% OF
WELDING AMPS
-
NO PULSE FUNCTION DIRECT AMP CONTROL RATIO CONTROLLED: 5-95% OF
WELDING AMPS
-
RATIO CONTROLLED:
5-95% OF WELDING
AMPS
DIRECT AMP CONTROL
PULSE TIME ON (WIDTH) RATIO CONTROLLED: 10-90% OF PULSE CYCLE NO PULSE FUNCTION RATIO CONTROLLED 10-90% OF PULSE CYCLE RATIO CONTROLLED 10-90% OF PULSE CYCLE RATIO CONTROLLED 10-90% OF PULSE CYCLE RATIO CONTROLLED 10-90 % OF PULSE CYCLE
* DIRECT AMP CONTROL WORKS DIFFERENTLY WITH THE FOOT PEDAL THAN RATIO CONTROLLED UNITS. WHEN USING THE FOOT PEDAL AND PULSE TOGETHER ON DIRECT AMP CONTROL PULSE UNITS, THE PEDAL WILL ONLY CONTROL THE MAIN AMP (BASE AMPS) VALUE. THE PULSE AMPS WILL REMAIN FIXED. INCREASING PEDAL TRAVEL WILL DECREASE PULSE AMP DIFFERENTIAL.

The EVERLAST PowerTig 225 LX is a popular choice for welders who work on a variety of projects. Portable and superbly designed, this product easily passes through otherwise restrictive openings such as pipes, the fuselage in an airplane other areas where compact size is a necessity.[read more...]

Visa Mastercard American Express Discover eCheck PayPal
Copyright 2004 - 2011 Everlast Power Equipment Inc. All Rights Reserved.

 

Diesel Generators | Multi-Purpose Units | Plasma Cutters | Welders | TIG Water Coolers | Welding Helmets | Consumables | Spare Parts | Accessories
Welders Word Press | Welders News | Sitemap | Welder Blog | Welding Equipment Blogspot | Welding Supply Articles | Welding Calculators
Welding Symbols | Welding Terms | Welding Terms Finder | Welders Schools


While welding is a valuable skill to possess, it is important to get the right machine to do the job. If you are a professional or a hobbyist and are trying to find the machine to fit your needs, Everlast can help. We offer a full line of welders for the hobbyist and professionals, including MIG, TIG, STICK and plasma cutters. We are proud to feature IGBT components and modules from Siemens for long life service whether in the field, in the shop or in the home. Don't forget about our line of silent diesel generators and engine drive welders. We offer convenient ordering capability without leaving your home or office.